🧪 Kimyoviy tarkibi
| Element | Tarkibi (%) |
|---|---|
| Uglerod (C) | 0,08 dan kam yoki unga teng |
| Marganets (Mn) | 2.00 dan kam yoki unga teng |
| Silikon (Si) | 0,75 dan kam yoki unga teng |
| Fosfor (P) | 0,045 dan kam yoki unga teng |
| Oltingugurt (S) | 0,030 dan kam yoki unga teng |
| Xrom (Cr) | 17.0 - 20.0 |
| Nikel (Ni) | 9.0 - 13.0 |
| Niobiy (Nb) | 10 × C min, 1,00 maksimal |
| Temir (Fe) | Balans |
⚙️ Mexanik xususiyatlari
| Mulk | Qiymat |
|---|---|
| Kuchlanish kuchi (xona harorati) | 515 MPa dan katta yoki unga teng |
| Hosildorlik (0,2% ofset) | 205 MPa dan katta yoki unga teng |
| 50 mm gacha cho'zish | 40% dan katta yoki teng |
| Qattiqlik (Brinell) | 217 HB dan kam yoki unga teng |
| Qattiqlik (Rokvell B) | 95 HRB dan kam yoki unga teng |
| Ta'sir energiyasi (Charpy V-cho'qqisi, 20 daraja) | 120 J dan katta yoki unga teng |
| Charchoq chegarasi (107tsikllar) | 240 MPa |
| Young moduli | 200 GPa |
🔬 Jismoniy xususiyatlar
| Mulk | Qiymat |
|---|---|
| Zichlik | 7,95 g/sm³ |
| Erish nuqtasi | 1400-1450 daraja |
| Issiqlik o'tkazuvchanligi (20 daraja) | 14.2 W/m·K |
| Issiqlik kengayish koeffitsienti (20-100 daraja) | 17.3×10-6/K |
| Maxsus issiqlik sig'imi | 500 J/kg·K |
| Elektr qarshiligi (20 daraja) | 0.73 µΩ·m |
| Magnit o'tkazuvchanlik | 1.02 (paramagnit) |
| Puasson nisbati | 0.27-0.30 |
📏 Mahsulot xususiyatlari
| Mahsulot shakli | Mavjud o'lchamlar | Standartlar |
|---|---|---|
| Issiq haddelenmiş plitalar | Qalinligi: 6-100 mm, kengligi: 2500 mm gacha | ASTM A240, ASME SA-240 |
| Sovuq haddelenmiş choyshablar | Qalinligi: 0,4-6 mm, kengligi: 1500 mm gacha | ASTM A240, EN 10088-2 |
| Dumaloq panjaralar | Diametri: 6-300 mm, Uzunligi: 6000 mm gacha | ASTM A276, ASTM A479 |
| Choksiz quvurlar | OD: 6-610 mm, WT: 1-60 mm | ASTM A213, ASTM A312 |
| Payvandlangan quvurlar | OD: 10-1220mm, WT: 1-40mm | ASTM A312, ASTM A358 |
| Yuzaki qoplamalar | 2B, BA, No.4, HL, Mirror | ASTM A480 |
| O'lchovli bardoshlik | ± 0,1 mm dan ± 0,5 mm gacha | ASTM standartlariga muvofiq |