🧪 Kimyoviy tarkibi

Element Tarkibi (%)
Uglerod (C) 0.04 - 0.10
Marganets (Mn) 2.00 dan kam yoki unga teng
Kremniy (Si) 0,75 dan kam yoki unga teng
Fosfor (P) 0,045 dan kam yoki unga teng
Oltingugurt (S) 0,030 dan kam yoki unga teng
Chromium (Cr) 17.0 - 20.0
Nikel (Ni) 9.0 - 13.0
Titan (Ti) 4×(C+N) min, 0,70 maks
Azot (N) 0,10 dan kam yoki unga teng
Temir (Fe) Balans

⚙️ Mexanik xususiyatlari

Mulk Qiymat
Kuchlanish kuchi (xona harorati) 515 MPa dan katta yoki unga teng
Hosildorlik (0,2% ofset) 205 MPa dan katta yoki unga teng
Cho'zilish (50 mm o'lchagich) 40% dan katta yoki teng
Hududning qisqarishi 50% dan katta yoki teng
Qattiqlik (Brinell) 217 HB dan kam yoki unga teng
Ta'sir energiyasi (Charpy V-cho'qqi, xona harorati) 68 J dan katta yoki unga teng
Young moduli 200 GPa
O'rmalanish kuchi (650 daraja da 100 000 soat) 35 MPa
Charchoq chegarasi (107tsikllar) 240 MPa

🔬 Jismoniy xususiyatlar

Mulk Qiymat
Zichlik 7,90 g/sm³
Erish nuqtasi 1400-1450 daraja
Issiqlik o'tkazuvchanligi (20 daraja) 16.3 W/m·K
Issiqlik o'tkazuvchanligi (100 daraja) 17.8 W/m·K
Termal kengayish (20-100 daraja) 17.2×10-6/K
Termal kengayish (20-500 daraja) 18.4×10-6/K
Maxsus issiqlik sig'imi 500 J/kg·K
Elektr qarshiligi (20 daraja) 0.72 µΩ·m
Magnit o'tkazuvchanlik 1,02 mkr (magnitsiz-)
Kyuri harorati Magnit bo'lmagan-

📏 Mahsulot xususiyatlari

Spetsifikatsiya Mavjud variantlar
Mahsulot shakllari Barlar, novdalar, plitalar, choyshablar, quvurlar, quvurlar, zarblar, quyma
Bar diametri diapazoni 6 mm - 300 mm
Plitalar qalinligi diapazoni 3mm - 150mm
Plitalar qalinligi diapazoni 0,5 mm - 6 mm
Quvurning tashqi diametri 6 mm - 219 mm
Standartlarga muvofiqligi ASTM A240, A479, A312, EN 10088-2, JIS G4304, GB/T 1220
Yuzaki qoplamalar Issiq haddelenmiş, sovuq haddelenmiş, 2B, BA, No.4, HL, oyna
O'lchovli bardoshlik ± 0,1 mm dan ± 0,5 mm gacha (shakl va o'lchamga qarab)
Uzunlik parametrlari Standart uzunliklar yoki mijozning spetsifikatsiyasiga muvofiq kesilgan