Gnee dan yuqori sifatli AISI 304H zanglamaydigan po'latdir
Mar 23, 2026
Xabar QOLDIRISH



🧪 Kimyoviy tarkibi
| Element | Tarkibi (%) |
|---|---|
| Uglerod (C) | 0.04 - 0.10 |
| Marganets (Mn) | 2.00 dan kam yoki unga teng |
| Kremniy (Si) | 0,75 dan kam yoki unga teng |
| Fosfor (P) | 0,045 dan kam yoki unga teng |
| Oltingugurt (S) | 0,030 dan kam yoki unga teng |
| Chromium (Cr) | 18.0 - 20.0 |
| Nikel (Ni) | 8.0 - 10.5 |
| Azot (N) | 0,10 dan kam yoki unga teng |
| Temir (Fe) | Balans |
⚙️ Mexanik xususiyatlari
| Mulk | Qiymat |
|---|---|
| Kuchlanish kuchi (min) | 515 MPa |
| Hosildorlik kuchi 0,2% ofset (min) | 205 MPa |
| 50 mm da cho'zilish (min) | 40% |
| Maydonni qisqartirish (min) | 50% |
| Qattiqlik (Brinell) | 201 HB dan kam yoki unga teng |
| Qattiqlik (Rockwell B) | 92 HRB dan kam yoki unga teng |
| Ta'sir energiyasi (Charpy V-20 gradusda) | 120 J dan katta yoki unga teng |
| Charchoq chegarasi (10^7 tsikl) | 240 MPa |
| Elastiklik moduli | 200 GPa |
🔬 Jismoniy xususiyatlar
| Mulk | Qiymat |
|---|---|
| Zichlik | 8,00 g/sm³ |
| Erish nuqtasi | 1400-1450 daraja |
| Issiqlik o'tkazuvchanligi (100 daraja) | 16.2 W/m·K |
| Issiqlik kengayish koeffitsienti (20-100 daraja) | 17.2×10-6/K |
| Maxsus issiqlik sig'imi | 500 J/kg·K |
| Elektr qarshiligi (20 daraja) | 0.72 µΩ·m |
| Magnit o'tkazuvchanlik | 1.02 (magnitsiz-) |
| Termal diffuziya | 4.2×10-6 m²/s |
| Kyuri harorati | Yo'q (Ostenitik) |
📏 Mahsulot xususiyatlari
| Spetsifikatsiya | Mavjud variantlar |
|---|---|
| Mahsulot shakllari | Plitalar, choyshablar, rulolar, barlar, novdalar, quvurlar, quvurlar, zarb qilingan buyumlar |
| Plitalar qalinligi | 6 mm - 200 mm |
| Plitalar qalinligi | 0,4 mm - 6 mm |
| Bar diametri | 6 mm - 300 mm |
| Quvurning tashqi diametri | 6 mm - 610 mm |
| Standartlar | ASTM A240, A479, A312, EN 10088-2, JIS G4305, GB/T 3280 |
| Yuzaki tugatish | 2B, BA, No.4, HL (Soch chizig'i), Mirror, Tuzlangan |
| Tolerantlik | ± 0,1 mm (qalinligi), ± 3 mm (kengligi), ± 6 mm (uzunligi) |
| Chet holati | Tegirmon qirrasi, qirrali qirrasi, kesilgan cheti |
| Issiqlik bilan ishlov berish | Tavlangan eritma (1040-1120 daraja) |
So'rov yuborish