🧪 Kimyoviy tarkibi
| Element | Tarkibi (%) |
|---|---|
| Uglerod (C) | 0,08 dan kam yoki unga teng |
| Marganets (Mn) | 2.00 dan kam yoki unga teng |
| Kremniy (Si) | 1,00 dan kam yoki unga teng |
| Fosfor (P) | 0,045 dan kam yoki unga teng |
| Oltingugurt (S) | 0,030 dan kam yoki unga teng |
| Chromium (Cr) | 17.0 - 20.0 |
| Nikel (Ni) | 9.0 - 12.0 |
| Titan (Ti) | 5×C min, 0,70 maks |
| Azot (N) | 0,10 dan kam yoki unga teng |
| Temir (Fe) | Balans |
⚙️ Mexanik xususiyatlari
| Mulk | Qiymat |
|---|---|
| Kuchlanish kuchi (xona harorati) | 515 MPa dan katta yoki unga teng |
| Hosildorlik (0,2% ofset) | 205 MPa dan katta yoki unga teng |
| Cho'zilish (50 mm o'lchagich) | 40% dan katta yoki teng |
| Hududning qisqarishi | 50% dan katta yoki teng |
| Qattiqlik (Brinell) | 217 HB dan kam yoki unga teng |
| Qattiqlik (Rockwell B) | 95 HRB dan kam yoki unga teng |
| Ta'sir energiyasi (Charpy V-cho'qqi, xona harorati) | 120 J dan katta yoki unga teng |
| Charchoq chegarasi (10 va 7 davr) | 240 MPa |
| Young moduli | 200 GPa |
| Kesish moduli | 81 GPa |
🔬 Jismoniy xususiyatlar
| Mulk | Qiymat |
|---|---|
| Zichlik | 7,90 g/sm³ |
| Erish nuqtasi | 1400-1425 daraja |
| Issiqlik o'tkazuvchanligi (100 daraja) | 16.3 W/m·K |
| Issiqlik o'tkazuvchanligi (500 daraja) | 21.5 W/m·K |
| Termal kengayish (20-100 daraja) | 16.6×10-6/K |
| Termal kengayish (20-500 daraja) | 17.8×10-6/K |
| Maxsus issiqlik (20 daraja) | 500 J/kg·K |
| Elektr qarshiligi (20 daraja) | 0.72 µΩ·m |
| Magnit o'tkazuvchanlik | 1,02 mkr (maksimal) |
| Kyuri harorati | Magnit bo'lmagan- |
📏 Mahsulot xususiyatlari
| Spetsifikatsiya | Mavjud variantlar |
|---|---|
| Mahsulot shakllari | Dumaloq novda, kvadrat bar, yassi novda, plastinka, varaq, tasma, quvur, quvur, sim, zarb |
| Dumaloq novda diametri | 6 mm - 300 mm |
| Plitalar qalinligi | 3mm - 100mm |
| Plitalar qalinligi | 0,5 mm - 6 mm |
| Quvurning tashqi diametri | 6 mm - 219 mm |
| Standartlar | ASTM A240, A276, A312, A479, EN 10088, JIS G4303, GB/T 1220 |
| Yuzaki tugatish | Issiq haddelenmiş, sovuq haddelenmiş, yorqin tavlangan, tuzlangan, 2B, BA, №4, HL |
| O'lchovli bardoshlik | ± 0,1 mm dan ± 0,5 mm gacha (shakl va o'lchamga qarab) |
| Uzunlik | Standart: 6m, Maxsus: 1m - 12m |
| Vaziyat | Tavlangan, ishlov berilgan eritma |