Standartlar va texnik xususiyatlar

ASTM A249 \/ A269 \/ A213

En 10217-7 \/ en {1}}

ISO 1127

Asme \/ ped \/ ad2 {{1} 00 w0 sertifikatlari mavjud

 

ASTM A249 \/ A269 \/ A213 kimyoviy tarkibi

Standart C (uglerod) Si (Silikon) Mn (marganets tili) P (fosfor) S (oltingugurt) Ni (nikel) CR (xromium) Mo (Malybdddy) N (azot)
304 (AsTM) 0 dan kam yoki teng}. 08 0 dan kam yoki teng. 75 2 dan kam yoki unga teng. 00 0 dan kam yoki teng}. 045 0 dan kam yoki teng}. 03 8.0 - 10.5 18.0 - 20.0 - 0 dan kam yoki teng}. 01
304l (AsTM) 0 dan kam yoki teng}. 03 0 dan kam yoki teng. 75 2 dan kam yoki unga teng. 00 0 dan kam yoki teng}. 045 0 dan kam yoki teng}. 03 8.0 - 12.0 18.0 - 20.0 - 0 dan kam yoki teng}. 01
316 (AsTM) 0 dan kam yoki teng}. 08 0 dan kam yoki teng. 75 2 dan kam yoki unga teng. 00 0 dan kam yoki teng}. 045 0 dan kam yoki teng}. 03 10.0 - 14.0 16.0 - 18.0 2.0 - 3.0 0 dan kam yoki teng}. 01
316l (Asti) 0 dan kam yoki teng}. 03 0 dan kam yoki teng. 75 2 dan kam yoki unga teng. 00 0 dan kam yoki teng}. 045 0 dan kam yoki teng}. 03 10.0 - 14.0 16.0 - 18.0 2.0 - 3.0 0 dan kam yoki teng}. 01
430 (AsTM) 0 dan kam yoki teng. 12 1 dan kam yoki teng. 00 1 dan kam yoki teng. 00 0 dan kam yoki teng}. 040 0 dan kam yoki teng}. 03 - 16.0 - 18.0 - -
Sys304 (jis) 0 dan kam yoki teng}. 08 1 dan kam yoki teng. 00 2 dan kam yoki unga teng. 00 0 dan kam yoki teng}. 045 0 dan kam yoki teng}. 03 8.0 - 10.5 18.0 - 20.0 - -
Sys304l (jis) 0 dan kam yoki teng}. 03 1 dan kam yoki teng. 00 2 dan kam yoki unga teng. 00 0 dan kam yoki teng}. 045 0 dan kam yoki teng}. 03 9.0 - 13.0 18.0 - 20.0 - -
Sys316 (jis) 0 dan kam yoki teng}. 08 1 dan kam yoki teng. 00 2 dan kam yoki unga teng. 00 0 dan kam yoki teng}. 045 0 dan kam yoki teng}. 03 10.0 - 14.0 16.0 - 18.0 2.0 - 3.0 -
Sys316l (jis) 0 dan kam yoki teng}. 03 1 dan kam yoki teng. 00 2 dan kam yoki unga teng. 00 0 dan kam yoki teng}. 045 0 dan kam yoki teng}. 03 12.0 - 16.0 16.0 - 18.0 2.0 - 3.0 -
Sys430 (jis) 0 dan kam yoki teng. 12 0 dan kam yoki teng. 75 1 dan kam yoki teng. 00 0 dan kam yoki teng}. 040 0 dan kam yoki teng}. 03 - 16.0 - 18.0 - -
06cr119ni10 (GB) 0 dan kam yoki teng}. 08 1 dan kam yoki teng. 00 2 dan kam yoki unga teng. 00 0 dan kam yoki teng}. 045 0 dan kam yoki teng}. 03 8.0 - 11.0 18.0 - 20.0 - -
022CR119Ni10 (GB) 0 dan kam yoki teng}. 03 1 dan kam yoki teng. 00 2 dan kam yoki unga teng. 00 0 dan kam yoki teng}. 045 0 dan kam yoki teng}. 03 8.0 - 12.0 18.0 - 20.0 - -
06cr117ni12Mo2 (GB) 0 dan kam yoki teng}. 08 1 dan kam yoki teng. 00 2 dan kam yoki unga teng. 00 0 dan kam yoki teng}. 045 0 dan kam yoki teng}. 03 10.0 - 14.0 16.0 - 18.0 2.0 - 3.0 -
022CR117Ni12Mo2 (GB) 0 dan kam yoki teng}. 03 1 dan kam yoki teng. 00 2 dan kam yoki unga teng. 00 0 dan kam yoki teng}. 045 0 dan kam yoki teng}. 03 10.0 - 14.0 16.0 - 18.0 2.0 - 3.0 -
10cr117 (GB) 0 dan kam yoki teng. 12 1 dan kam yoki teng. 00 1 dan kam yoki teng. 00 0 dan kam yoki teng}. 040 0 dan kam yoki teng}. 03 - 16.0 - 18.0 - -
X5CRNI 18 - 10 (1.4301, EN) 0.07 1 dan kam yoki teng. 00 2 dan kam yoki unga teng. 00 0 dan kam yoki teng}. 045 0 dan kam yoki teng}. 015 8.0 - 10.5 17.5 - 19.5 - 0 dan kam yoki teng. 11
X2CRNI 18 - 9 (1.4307, EN) 0.03 1 dan kam yoki teng. 00 2 dan kam yoki unga teng. 00 0 dan kam yoki teng}. 045 0 dan kam yoki teng}. 015 8.0 - 10.0 17.5 - 19.5 - 0 dan kam yoki teng. 11
X5Crnimamo 17 - 12 - 2 (1.4401, EN) 0.07 1 dan kam yoki teng. 00 2 dan kam yoki unga teng. 00 0 dan kam yoki teng}. 045 0 dan kam yoki teng}. 015 10.0 - 13.0 16.5 - 18.5 2.0 - 3.0 0 dan kam yoki teng. 11
X2Crnimamo 17 - 12 - 2 (1.4404, EN) 0.03 1 dan kam yoki teng. 00 2 dan kam yoki unga teng. 00 0 dan kam yoki teng}. 045 0 dan kam yoki teng}. 015 10.0 - 13.0 16.5 - 18.5 2.0 - 3.0 0 dan kam yoki teng. 11
X5CRUMO 17 - 12 - 2 (1.4406, EN) 0.07 1 dan kam yoki teng. 00 2 dan kam yoki unga teng. 00 0 dan kam yoki teng}. 045 0 dan kam yoki teng}. 015 10.0 - 13.0 16.5 - 18.5 2.0 - 2.5 0 dan kam yoki teng. 11

Qozonsiz issiqlik almashtirgichlari va kondensatorlarning sirtni davolash uchun zanglamaydigan po'lat naychalar

Buyum Sirtmoq Dumaloq naycha - astm standarti
  Mf Payvandlanganidek
  180# 180 # yalang'och parlatishdan keyin
  400# Parlatishdan keyin 400 #
  600# 600 # yalang'och holda parlatishdan keyin bufer
  Hl Soch chizig'i 180 # \/ 240 # ni parlatishdan keyin tugadi
Kvadrat va to'rtburchaklar naycha Mf Payvandlanganidek
  180# 180 # yalang'och parlatishdan keyin
  400# Parlatishdan keyin 400 #
  600# 600 # yalang'och holda parlatishdan keyin bufer
  Hl Soch chizig'i 180 # \/ 240 # ni parlatishdan keyin tugadi
  Yo'q.3 100 - 120 # abraziv kamar bilan sayqallanadi
  №4 150 - 180 # abraziv kamar bilan sayqallanadi
  Hl 150 - 320 # abraziv kamar silliqlash, chiziqli naqsh

 

ASTM A249 \/ A269 \/ A213 E 10217-7

Qalinligi \/ mm 0.80 1.00 1.20 1.24 1.50 1.65 2.00 2.11 2.50 3.00 3.50
O'lchov (dyuym)     18 gaga 16 gaga 16 gaga   14ga   12 gaga   11ga
9.50 (3/8)      
12.70 (1/2)      
15.90 (5/8)      
16.00      
18.00      
19.10 (3/4)      
21.34      
22.00      
22.25 (7/8)      
25.00      
25.40 (1)      
26.67      
28.58 (1 1/8)      
31.80 (1 1/4)      
32.00      
33.40      
34.00      
35.00      
38.10 (1 1/2)    
40.00    
41.30    
42.70    
44.50 (1 3/4)    
48.26    
48.60    
50.80 (2)    
52.00    
57.00    
60.33    
63.00 (2 1/2)    
70.00    
76.20 (3)    
85.00    
89.00 (3 1/2)    
101.60 (4)    
104.30    
114.30 (4 1/2)    

Afsona:

☆ A249 \/ A269 jarayonini ifodalaydi

○ A269 jarayonini anglatadi

△ A249 \/ A269 jarayonini taqdim etadi

Faqat boncuk ichdi

 

Qozondagi issiqlik almashinuvchi va kondensisterlar uchun zanglamaydigan po'lat naychalar

Stainless Steel Tubes For Boiler Heat Exchangers And Condensers In Stock

Mahsulotni qo'llash:Yuqori bosimli elektr stantsiyalari, g'ayritabiiy quvurlar, qaynoq suv quvurlari va qaynoq suv quvurlari qurilishi.

 

Sinov va sertifikatlar

100% Eddy hozirgi \/ gidrostatik test

PMI (materiallarni tekshirish)

ISO 9001: 2015 sifat nazorati

Pe \/ reklama 2 {{1} 00 w0 \/ asme \/ cpre11090

3.1 \/ 3,2 mln. Test sinovlari

 