Xitoydan yuqori sifatli AISI 316H zanglamaydigan po'lat

Apr 08, 2026

Xabar QOLDIRISH

What are the properties of 1.4568 material?What is 1.4568 stainless steel equivalent to?What is 1.4568 Stainless Steel?What is 1.4521 Stainless Steel?

🧪 Kimyoviy tarkibi

Element Tarkibi (%)
Uglerod (C) 0.04 - 0.10
Marganets (Mn) 2.00 dan kam yoki unga teng
Kremniy (Si) 0,75 dan kam yoki unga teng
Fosfor (P) 0,045 dan kam yoki unga teng
Oltingugurt (S) 0,030 dan kam yoki unga teng
Chromium (Cr) 16.0 - 18.0
Nikel (Ni) 10.0 - 14.0
Molibden (Mo) 2.0 - 3.0
Azot (N) 0,10 dan kam yoki unga teng
Temir (Fe) Balans

⚙️ Mexanik xususiyatlari

Mulk Qiymat
Kuchlanish kuchi (xona harorati) 515 MPa dan katta yoki unga teng
Hosildorlik (0,2% ofset) 205 MPa dan katta yoki unga teng
Cho'zilish (50 mm o'lchagich) 40% dan katta yoki teng
Hududning qisqarishi 50% dan katta yoki teng
Qattiqlik (Brinell) 217 HB dan kam yoki unga teng
Qattiqlik (Rockwell B) 95 HRB dan kam yoki unga teng
Ta'sir energiyasi (Charpy V-cho'qqisi, 20 daraja) 120 J dan katta yoki unga teng
Charchoq chegarasi (107tsikllar) 240 MPa
Young moduli 200 GPa
Kesish moduli 81 GPa

🔬 Jismoniy xususiyatlar

Mulk Qiymat
Zichlik (20 daraja) 8,0 g/sm³
Erish nuqtasi 1400-1450 daraja
Issiqlik o'tkazuvchanligi (20 daraja) 16.2 W/m·K
Issiqlik o'tkazuvchanligi (100 daraja) 17.5 W/m·K
Termal kengayish (20-100 daraja) 16.0×10-6/K
Termal kengayish (20-300 daraja) 17.0×10-6/K
Maxsus issiqlik (20 daraja) 500 J/kg·K
Elektr qarshiligi (20 daraja) 0.74 µΩ·m
Magnit o'tkazuvchanlik 1,02 mkr (maksimal)
Kyuri harorati Magnit bo'lmagan-

📏 Mahsulot xususiyatlari

Spetsifikatsiya Mavjud variantlar
Mahsulot shakllari Dumaloq barlar, tekis barlar, plitalar, choyshablar, quvurlar, quvurlar, zarblar, to'qimalar
Dumaloq novda diametri 6 mm - 300 mm
Yassi novda o'lchamlari 10×3mm - 150×50mm
Plitalar qalinligi 3mm - 100mm
Plitalar qalinligi 0,5 mm - 3 mm
Quvurning tashqi diametri 6 mm - 219 mm
Standartlarga muvofiqligi ASTM A240, A276, A312, A479, EN 10088, JIS G4303, GB/T 1220
Yuzaki qoplamalar Issiq haddelenmiş, sovuq tortilgan, yorqin tavlangan, tuzlangan, sayqallangan (2B, BA, №4)
O'lchovli bardoshlik ± 0,1 mm dan ± 0,5 mm gacha (mahsulot shakliga qarab)
Uzunlik parametrlari Standart uzunliklar: 3m, 6m, 12m; Maxsus uzunliklar mavjud