ASTM A312 316L Stainless Steel Seamless Pipe 1.4404 StainlessSteel Pipe Custom Cutting SS PipeASTM A312 TP310S Stainless Steel Seamless Tube DIN1.4845 SS Pipe For High TemperatureWhat is 1.4720 Stainless Steel?

 

 

 

🧪 Kimyoviy tarkibi

Element Tarkibi (%)
Uglerod (C) 0,030 dan kam yoki unga teng
Marganets (Mn) 2.00 dan kam yoki unga teng
Kremniy (Si) 0,75 dan kam yoki unga teng
Fosfor (P) 0,045 dan kam yoki unga teng
Oltingugurt (S) 0,030 dan kam yoki unga teng
Chromium (Cr) 16.00 - 18.00
Nikel (Ni) 10.00 - 14.00
Molibden (Mo) 2.00 - 3.00
Azot (N) 0,10 dan kam yoki unga teng
Temir (Fe) Balans

⚙️ Mexanik xususiyatlari

Mulk Qiymat
Kuchlanish kuchi (Rm) 485 - 620 MPa
Hosildorlik (Rp0,2) 205 MPa dan katta yoki unga teng
Cho'zilish (A50 mm) 40% dan katta yoki teng
Qattiqlik (HRB) 95 dan kam yoki teng
Qattiqlik (HV) 200 - 250
Ta'sir energiyasi (KV) 60 J dan katta yoki unga teng (20 darajada)
Young moduli 200 GPa
Charchoq chegarasi 245 MPa (107tsikllar)
Puasson nisbati 0.27 - 0.30