Kimyoviy xossalari

 

  C Mn Si P S Cr Mo Ni N
316 (S31600) 0,08 maksimal 2,0 maks 0,75 maks 0,045 maks 0,03 maksimal

min: 16.0

maksimal: 18.0

min: 2.0

maksimal: 3.0

min: 10,0

maksimal: 14.0

0,10 maks
316L (S31603) 0,03 maksimal 2,0 maks 0,75 maks 0,045 maks 0,03 maksimal

min: 16.0

maksimal: 18.0

min: 2.0

maksimal: 3.0

min: 10,0

maksimal: 14.0

0,10 maks

 

 

Mexanik xususiyatlar

 

Baho Kuchlanish kuchi ksi (min) Hosildorlik kuchi 0,2% ksi (min) Uzayish % Qattiqlik (Brinell) MAX Qattiqlik (Rokvell B) MAX

316

(S31600)

75 30 40 217 95

316L

(S31603)

70 25 40 217 95

 

 

Jismoniy xususiyatlar

 

Zichlik lbm/in3 Issiqlik o'tkazuvchanligi (BTU/soat fut F daraja) Elektr qarshiligi (x 10-6 da) Elastiklik moduli (psi x 10-6) Issiqlik kengayish koeffitsienti (in/in)/ F x 10-6 darajasi) Maxsus issiqlik (BTU/lb/ F daraja) Erish diapazoni (F darajasi)
68 daraja F da 0,29 68 212 F darajasida 100,8 68 daraja F da 29,1 29 32 - 212 daraja 8,9 68 daraja F da 0,108 2500 dan 2550 gacha
        32 - 1000 gradusda 9,7 200 daraja F da 0,116  
        11,1 32 - 1500 daraja    