440 zanglamaydigan po'lat nima?
Feb 24, 2026
Xabar QOLDIRISH



440 zanglamaydigan po'latdan yasalgan plastinkaning ekvivalent materiali
440A zanglamaydigan po'latdan:
Ekvivalent AISI 440A, ASTM A276, ASTM A314, ASTM A473, ASTM A580, ASTM A756, ASTM A580, AMS 5631, AMS 5632, AMS 5633, AMS 5634, AMS28S, AMS28, {0}-{101} SAE J405 (51440A)
Shunga o'xshash navlar: 7Cr17, 7Cr17MoV, X70CrMo15
440B zanglamaydigan po'latdan:
Ekvivalent AISI 440B, ASTM A276, ASTM A314, ASTM A473, ASTM A580, ASTM A756, ASTM A580, AMS 5631, AMS 5632, AMS 5633, AMS 5634, AMS28S, AMS28, {0}-{101} SAE J405 (51440B)
Shunga o'xshash navlar: 9Cr18, 9Cr18Mo, X90CrMoV18
440C zanglamaydigan po'latdan:
AISI 440C, ASTM A276, ASTM A314, ASTM A473, ASTM A580, ASTM A756, ASTM A580, AMS 5630, AMS 5880, MIL-S-862, SAE J140C (SAE J140C) ga ekvivalent
Shunga o'xshash navlar: 9Cr18MoV, X105CrMo17
440 zanglamaydigan po'latdan yasalgan plastinkaning kimyoviy tarkibi (%)
| Baho | C | Si | Mn | S | P | Cr | Ni | Mo |
|---|---|---|---|---|---|---|---|---|
| 440A | 0.60~0.75 | 1 dan kichik yoki teng | 1 dan kichik yoki teng | 0,030 dan kam yoki unga teng |
0,040 dan kam yoki unga teng |
16.00-18.00 | – | 0,75 dan kam yoki unga teng |
| 440B | 0.85-0.95 | 1 dan kichik yoki teng | 1 dan kichik yoki teng | 0,030 dan kam yoki unga teng | 0,035 dan kam yoki unga teng | 16.00-18.00 | 0,60 dan kam yoki unga teng | 0,75 dan kam yoki unga teng |
| 440C | 0.95 – 1.20 | 1 dan kichik yoki teng | 1 dan kichik yoki teng | 0,030 dan kam yoki unga teng | 0,040 dan kam yoki unga teng | 16.00-18.00 | – | 0,75 dan kam yoki unga teng |
Mexanik xususiyatlar
| Mulk | 440A | 440B | 440C |
|---|---|---|---|
| Qattiqlik (Rokvell C) | 56-59 HRC | 57-60 HRC | 58-62 HRC |
| Kuchlanish kuchi (MPa) | 760-820 | 760-840 | 760-820 |
| Kuchlanish kuchi (MPa) | 450-600 | 450-600 | 450-600 |
| Uzilish cho'zilishi (%) | 20-25 | 15-20 | 10-15 |
| Elastiklik moduli (GPa) | 200 | 200 | 200 |
Jismoniy xususiyatlar
| Mulk | 440A | 440B | 440C |
|---|---|---|---|
| Zichlik (g/sm³) | 7.65 | 7.75 | 7.75 |
| Issiqlik o'tkazuvchanligi (Vt/m·K) | 24 | 24 | 24 |
| Maxsus issiqlik sig'imi (J/kg·K) | 460 | 460 | 460 |
| Elektr qarshiligi (mk·sm) | 60 | 60 | 60 |
| Issiqlik kengayish koeffitsienti (mkm / m · K) | 10.4 | 10.4 | 10.4 |
So'rov yuborish