| Tavsif | 304 yozing |
|---|---|
| Ishonchli stress 0,2% (MPa) | 205 |
| Kuchlanish kuchi (MPa) | 515 |
| Cho'zilish A5 (%) | 40 |
| Qattiqlik | HB: 201 HRB: 92 |
Kimyoviy tarkibi
| . | . |
|---|---|
| UNS raqami | S30400 |
| UZ | 1.4301 |
| AISI | 304 |
| Uglerod (C) | 0.07 |
| Kremniy (Si) | 0.75 |
| Marganets (Mn) | 2.00 |
| Fosfor (P) | 0.045 |
| Oltingugurt (S) | 0.030 |
| Xrom (Cr) | 17.50 - 19.50 |
| Molibden (Mo) | |
| Nikel (Ni) | 8.00 - 10.50 |
| Azot (N) | 0.10 |