SUS347 zanglamaydigan po'lat: Niobiy-Yuqori harorat uchun barqarorlashtirilgan

Jan 28, 2026

Xabar QOLDIRISH

316 Stainless Steel Round BarWhat Is 316Ti (UNS S31635) Stainless SteelWhat Is 347 (UNS S34700) Stainless Steel

347 ekvivalent baholar

 

ASTM JIS UNS UZ DIN GOST GB

347

SUS347

S34700

1.4550

X6CrNiNb18-10

08Х18Н12Б

06Cr18Ni11Nb

 

 

Kimyoviy tarkibi

 

Baho Standart C (%) Cr (%) Ni (%) Nb+Ta (%) Mn (%) Si (%) P (%) S (%) Fe (%)

347

ASTM A240

0,08 dan kam yoki unga teng

17.0–19.0

9.0–13.0

10×C–1.0

2,0 dan kam yoki unga teng

1,0 dan kam yoki unga teng

0,045 dan kam yoki unga teng

0,03 dan kam yoki teng

Balans

1.4550

EN 10088-2

0,08 dan kam yoki unga teng

17.0–19.0

9.0–13.0

8×C–1.0

2,0 dan kam yoki unga teng

1,0 dan kam yoki unga teng

0,045 dan kam yoki unga teng

0,03 dan kam yoki teng

Balans

SUS347

JIS G 4304
JIS G 4305

0,08 dan kam yoki unga teng

17.0–19.0

9.0–13.0

8×C–1.0

2,0 dan kam yoki unga teng

1,0 dan kam yoki unga teng

0,045 dan kam yoki unga teng

0,03 dan kam yoki teng

Balans

 

 

Mexanik xususiyatlar

 

Baho Standart Mustahkamlik chegarasi Hosildorlik kuchi Cho'zilish Qattiqlik

347

ASTM A240

520 MPa dan katta yoki unga teng

205 MPa dan katta yoki unga teng

40% dan katta yoki teng

95 MPa dan kam yoki unga teng

1.4550

EN 10088-2

520 MPa dan katta yoki unga teng

205 MPa dan katta yoki unga teng

40% dan katta yoki teng

95 MPa dan kam yoki unga teng

SUS347

JIS G4304/4305

520 MPa dan katta yoki unga teng

205 MPa dan katta yoki unga teng

40% dan katta yoki teng

95 MPa dan kam yoki unga teng