SUS310S zanglamaydigan po'lat: Yuqori-haroratning korroziyaga chidamliligi

Jan 05, 2026

Xabar QOLDIRISH

Comparison Of SUS321 And SUS347: Titanium-Stabilized Vs Niobium-Stabilized Austenitic Stainless SteelComparison Of SUS316 And SUS316L: Standard Molybdenum-Containing Vs Low-Carbon Molybdenum-Containing Austenitic Stainless SteelComparison Of SUS304 And SUS316: General-Purpose Vs Molybdenum-Containing Corrosion-Resistant Austenitic Stainless Steel

Kimyoviy birikmalar

Element % Hozir (mahsulot shaklida)
  C, H, P, L TW* / TS*
Uglerod (C) 0,10 dan kam yoki unga teng 0,15 dan kam yoki unga teng
Kremniy (Si) 1,50 dan kam yoki unga teng 0,75 dan kam yoki unga teng
Marganets (Mn) 2.00 dan kam yoki unga teng 2.00 dan kam yoki unga teng
Fosfor (P) 0,045 dan kam yoki unga teng 0,045 dan kam yoki unga teng
Oltingugurt (S) 0,015 dan kam yoki unga teng 0,030 dan kam yoki unga teng
Xrom (Cr) 24.00 - 26.00 24.00 - 26.00
Nikel (Ni) 19.00 - 22.00 19.00 - 22.00
Azot (N) 0,11 dan kam yoki unga teng -
Temir (Fe) Balans Balans

So'rov yuborish