SUS304 zanglamaydigan po'latdan: korroziyaga qarshilik bo'yicha qo'llanma

Jan 06, 2026

Xabar QOLDIRISH

630 (17-4 PH) vs 15-5 PH (XM-12) Precipitation-Hardening Stainless Steels: Versatile vs High-Toughness Strength410 vs 430 Martensitic vs Ferritic Stainless Steels: Weldable Strength vs Decorative Cost-Effectiveness309S vs 310S Austenitic Stainless Steels: High-Temp Oxidation vs Extreme Heat Resistance

Zanglamaydigan po'latdan kimyoviy tarkibi 304

1-jadval.304 zanglamaydigan po'latdan yasalgan qotishmalar uchun kimyoviy tarkibi

%

304

304L

304H

C

0.0 - 0.07

0.0 - 0.03

0.04 - 0.08

Mn

0.0 - 2.0

0.0 - 2.00

0.0 - 2.0

Si

0.0 - 1.00

0.0 - 1.00

0.0 - 1.0

P

0.0 - 0.05

0.0 - 0.05

0.0 - 0.04

S

0.0 - 0.03

0.0 - 0.02

0.0 - 0.02

Cr

17.50 - 19.50

17.50 - 19.50

17.00 - 19.00

Ni

8.00 - 10.50

8.00 - 10.50

8.00 - 11.00

Fe

Balans

Balans

Balans

N

0.0-0.11

0.0-0.11

0.0 - 0.10

 

Zanglamaydigan po'lat 304 turli xil muhitlarda va turli xil korroziy vositalar bilan aloqa qilganda mukammal korroziyaga chidamliligiga ega. Xloridlar bo'lgan muhitda chuqurchalar va yoriqlar korroziyasi paydo bo'lishi mumkin. Stressli korroziya yorilishi 60 darajadan yuqori haroratlarda sodir bo'lishi mumkin.

 

So'rov yuborish