Super Dupleks zanglamaydigan po'lat
Jan 26, 2026
Xabar QOLDIRISH



Kimyoviy tarkibi
| Element | Tarkibi (%) |
|---|---|
| Uglerod (C) | 0,030 dan kam yoki unga teng |
| Xrom (Cr) | 24.0 - 26.0 |
| Nikel (Ni) | 6.0 - 8.0 |
| Molibden (Mo) | 3.0 - 4.0 |
| Volfram (Vt) | 0.5 - 1.0 |
| Azot (N) | 0.24 - 0.32 |
| Marganets (Mn) | 1,20 dan kam yoki unga teng |
| Kremniy (Si) | 0,80 dan kam yoki unga teng |
⚙️ Mexanik xususiyatlari
| Mulk | Qiymat |
|---|---|
| Hosildorlik kuchi (MPa) | 550 dan katta yoki teng |
| Kuchlanish kuchi (MPa) | 750 - 950 |
| Uzayish (%) | 25 dan katta yoki teng |
| Qattiqlik (HRC) | 32 dan kichik yoki teng |
| Kritik chuqurlik harorati (daraja) | 80 dan katta yoki teng |
| PREN qiymati | 40 dan katta yoki teng |
| Ta'sir energiyasi -40 daraja (J) | 60 dan katta yoki teng |