Zanglamaydigan po'latdan 310S darajasi - super issiqlikka chidamli daraja

Mar 23, 2026

Xabar QOLDIRISH

304 Stainless Steel Sheet for Food-Grade ApplicationsUNS S30409 Stainless Steel – High-Temperature Creep-Resistant 304 VariantUNS S30400 Stainless Steel – General-Purpose Corrosion-Resistant Core Alloy

Standartlar va ekvivalent baholar

ASTMJISUNSUZDINGOSTGB

310S

SUS310S

S31008

1.4845

X8CrNi25-21

20Х23Н18

0Cr25Ni20

Kimyoviy tarkibi 310S issiqlikka chidamli-

BahoStandartCCrNiMnSiPSMoFe

310S

ASTM A240

≤0,08

24,0–26,0

19,0–22,0

≤2,0

≤1,5

≤0,045

≤0,030

-

Balans

1.4845

EN 10088-2

≤0,08

24,0–26,0

19,0–22,0

≤2,0

≤1,5

≤0,045

≤0,030

-

Balans

SUS310S

JIS G 4304
JIS G 4305

≤0,08

24,0–26,0

19,0–22,0

≤2,0

≤1,5

≤0,045

≤0,030

-

Balans

AISI 310S ning mexanik xususiyatlari

310S zanglamaydigan po'lat yuqori haroratlarda barqarorlikni saqlab, yuqori kuchlanish va ajoyib o'rmalanish qarshiligini ta'minlaydi. Uning pastroq uglerod miqdori yaxshi payvandlanishini ta'minlaydi, etarli egiluvchanligi esa o'choq qismlari, issiqlik almashtirgichlar va sanoat uskunalari uchun ishonchli ishlab chiqarish imkonini beradi.

BahoStandartMustahkamlik chegarasiHosildorlik kuchiCho'zilishQattiqlik

310S

ASTM A240

≥520 MPa

≥205 MPa

≥40%

≤217 HBW

1.4845

EN 10088-2

≥520 MPa

≥210 MPa

≥40%

≤217 HBW

SUS310S

JIS G 4304
JIS G 4305

≥520 MPa

≥205 MPa

≥40%

≤217 HBW

So'rov yuborish