SS316 va SUS316 zanglamaydigan po'latdan: farqlar
Dec 03, 2025
Xabar QOLDIRISH
SS316 va SUS316 zanglamaydigan po'latdan: farqlar

SS316 uchun ekvivalent materiallar qanday?
SS316 zanglamaydigan po‘lat uchun ekvivalent materiallarga AQSHdan UNS S31600, Yevropa Ittifoqidan EN 1.4401 va X5CrNiMo17-12-2 hamda Buyuk Britaniyadan BS 316S31 va BS 316S33 kiradi. Cast SS316 ko'pincha CF8M deb ataladi. Bu molibden{15}}ostenitik xrom-nikel zanglamaydigan po'latdan iborat bo'lib, ayniqsa, xloridga boy muhitda korroziyaga mukammal qarshilik ko'rsatadi. Bu uni dengiz uskunalari, kimyoviy ishlov berish, oziq-ovqat va farmatsevtika ishlab chiqarish kabi ilovalar uchun ideal qiladi.
SUS316 ning ma'nosi nima?
SUS316 ostenitik zanglamaydigan po'latdir, korroziyaga mukammal qarshilik ko'rsatadi. Molibden qo'shilishi uning korroziyaga chidamliligini yanada oshiradi. 304 zanglamaydigan po'latdan, ayniqsa qirg'oqbo'yi hududlari yoki kimyoviy ishlov berish zavodlari kabi og'ir muhitda chuqurlik va korroziyaga nisbatan ancha chidamli. SUS316 juda yuqori unumdorlik va chidamlilik talablari boʻlgan ilovalar uchun mos keladigan koʻp qirrali va yuqori samarali materialdir.


SS316 va SUS316 zanglamaydigan po'latdan: farqlar
SS316 va SUS316 o'rtasida hech qanday farq yo'q; atamalar shunchaki bir xil zanglamaydigan po'lat uchun turli mintaqaviy belgilar bo'lib, "SS" Amerika qisqartmasi va "SUS" Yaponiya sanoat standartlari (JIS) "po'latdan foydalanish zanglamaydigan" belgisidir. Ikkala belgi ham molibden qo'shilishi tufayli yuqori korroziyaga chidamliligi bilan mashhur ostenitik zanglamaydigan po'lat bo'lgan bir xil 316 toifali qotishmaga tegishli.
|
Baho |
Standart tizim | Umumiy foydalanish hududi |
|---|---|---|
| SUS316 | JIS (Yaponiya) | Yaponiya, Koreya, ba'zi Xitoy tegirmonlari |
| SS316 | AISI / ASTM (AQSh) | Global foydalanish (ASTM A240, A213) |
| SS316L | AISI / ASTM (AQSh) | SS316 ning past-uglerodli versiyasi |
Kimyoviy tarkibi
| Element | SUS316 / SS316 (%) | SS316L (%) |
|---|---|---|
| Chromium | 16.0 – 18.0 | 16.0 – 18.0 |
| Nikel | 10.0 – 14.0 | 10.0 – 14.0 |
| Molibden | 2.0 – 3.0 | 2.0 – 3.0 |
| Uglerod | 0,08 dan kam yoki unga teng | 0,03 dan kam yoki unga teng (past uglerod) |
Mexanik xususiyatlar
| Mulk | SUS316 / SS316 | SS316L |
|---|---|---|
| Kuchlanish kuchi (Rm) | 515 - 750 MPa | 485 - 700 MPa |
| Hosildorlik (Rp0,2) | 205 MPa dan katta yoki unga teng | 170 MPa dan katta yoki unga teng |
| Cho'zilish | 40% dan katta yoki teng | 45% dan katta yoki teng |
| Qattiqlik (HB) | 217 dan kichik yoki teng | 217 dan kichik yoki teng |
316 va 316L zanglamaydigan po'latdan qanday farqlar bor?
Asosiy farq uglerod tarkibida 316L (<0.03%), which is significantly lower than that of 316 (<0.08%), making it more resistant to intergranular corrosion after welding. While both stainless steels are high-strength and corrosion-resistant, 316 is better suited for high-temperature applications due to its higher strength, while 316L is the preferred choice for projects requiring extensive welding.
SUS316 zanglamaydigan po'latning kamchiliklari qanday?
316 zanglamaydigan po'latning asosiy kamchiliklari 304 kabi navlarga nisbatan yuqori xarajat, past ishlov berish va shakllantirilishi va sezuvchanlik kabi potentsial payvandlash muammolari. Bundan tashqari, u bosim ostida yirtilib ketishga moyil va boshqa materiallarga nisbatan juda yuqori{3}}stressli ilovalar uchun unchalik yaxshi emas.
Dengiz, kimyo yoki sanoat loyihangiz uchun SS316/SUS316 zanglamaydigan po'latni qidiryapsizmi? Zanglamaydigan po'latdan barcha ehtiyojlaringiz uchun bepul narxlar, moslashtirilgan yechimlar va professional yordam olish uchun bugun GNEE bilan bog'laning.
SS316 zanglamaydigan po'latdan yasalgan plastinka mahsulot shakllari
Qalinligi: 2,0 mm dan 50 mm gacha
Kengligi: 1500 / 2000 mm gacha
Tugatish: 2B, No1, No4, HL, oyna
Standartlar: ASTM A240, JIS G4304, EN 10088-2
Sertifikatlar: EN 10204 3.1, NACE MR0175, PED



So'rov yuborish