🧪 Kimyoviy tarkibi
| Element | Tarkibi (%) |
|---|---|
| Uglerod (C) | 0,030 dan kam yoki unga teng |
| Kremniy (Si) | 1,00 dan kam yoki unga teng |
| Marganets (Mn) | 2.00 dan kam yoki unga teng |
| Fosfor (P) | 0,045 dan kam yoki unga teng |
| Oltingugurt (S) | 0,030 dan kam yoki unga teng |
| Chromium (Cr) | 17.0 - 20.0 |
| Nikel (Ni) | 10.0 - 15.0 |
| Molibden (Mo) | 2.0 - 3.0 |
| Azot (N) | 0,10 dan kam yoki unga teng |
| Temir (Fe) | Balans |
⚙️ Mexanik xususiyatlari
| Mulk | Qiymat |
|---|---|
| Kuchlanish kuchi (Rm) | 520 - 670 MPa |
| Hosildorlik (Rp0,2) | 220 MPa dan katta yoki unga teng |
| Uzayish (A5) | 40% dan katta yoki teng |
| Qattiqlik (HB) | 215 dan kichik yoki teng |
| Qattiqlik (HV) | 230 dan kam yoki unga teng |
| Ta'sir energiyasi (KV) 20 daraja | 60 J dan katta yoki unga teng |
| Young moduli | 200 GPa |
| Kesish moduli | 81 GPa |
| Puasson nisbati | 0.28 |
| Charchoq chegarasi (107tsikllar) | 240 MPa |
🔬 Jismoniy xususiyatlar
| Mulk | Qiymat |
|---|---|
| Zichlik | 8,0 g/sm³ |
| Erish nuqtasi | 1400 - 1450 daraja |
| Termal kengayish (20-100 daraja) | 16.0×10-6/K |
| Termal kengayish (20-200 daraja) | 16.5×10-6/K |
| 20 daraja issiqlik o'tkazuvchanligi | 15 W/m·K |
| 100 daraja issiqlik o'tkazuvchanligi | 16.3 W/m·K |
| Maxsus issiqlik sig'imi | 500 J/kg·K |
| Elektr qarshiligi 20 daraja | 0.75 µΩ·m |
| Magnit o'tkazuvchanlik | 1,02 mkr dan kam yoki unga teng |
| Kyuri harorati | Magnit bo'lmagan- |
📏 Mahsulot xususiyatlari
| Spetsifikatsiya | Mavjud variantlar |
|---|---|
| Mahsulot shakllari | Plitalar, plitalar, barlar, novdalar, quvurlar, quvurlar, rulolar, chiziqlar |
| Plitalar qalinligi | 0.3 - 6.0 mm |
| Plitalar qalinligi | 6.0 - 100 mm |
| Bar diametri | 6 - 300 mm |
| Quvurning tashqi diametri | 6 - 610 mm |
| Yuzaki qoplamalar | 2B, BA, No.4, HL, Mirror, Tuzlangan |
| Standartlar | EN 10088, ASTM A240/A276/A312, JIS G4305, GB/T 3280 |
| O'lchovli bardoshlik | ±0,1 mm (qalinligi), ±2 mm (kengligi) |
| Uzunlik | 2000 - 6000 mm (standart), Maxsus uzunliklar mavjud |
| Chet holati | Tegirmon qirrasi, qirrali qirrasi, kesilgan cheti |
So'rov yuborish