🧪 Kimyoviy tarkibi
| Element | Tarkibi (%) |
|---|---|
| Uglerod (C) | 0,030 dan kam yoki unga teng |
| Marganets (Mn) | 2.00 dan kam yoki unga teng |
| Kremniy (Si) | 0,75 dan kam yoki unga teng |
| Fosfor (P) | 0,045 dan kam yoki unga teng |
| Oltingugurt (S) | 0,030 dan kam yoki unga teng |
| Chromium (Cr) | 18.00 - 20.00 |
| Nikel (Ni) | 8.00 - 12.00 |
| Azot (N) | 0,10 dan kam yoki unga teng |
| Temir (Fe) | Balans |
⚙️ Mexanik xususiyatlari
| Mulk | Qiymat |
|---|---|
| Mustahkamlik chegarasi | 515 MPa dan katta yoki unga teng |
| Hosildorlik (0,2% ofset) | 205 MPa dan katta yoki unga teng |
| 50 mm gacha cho'zish | 40% dan katta yoki teng |
| Hududning qisqarishi | 50% dan katta yoki teng |
| Qattiqlik (Brinell) | 200 HB dan kam yoki unga teng |
| Qattiqlik (Rockwell B) | 90 HRB dan kam yoki unga teng |
| Ta'sir energiyasi (Charpy V-20 gradusda) | 120 J dan katta yoki unga teng |
| Charchoq chegarasi (107tsikllar) | 240 MPa |
| Elastiklik moduli | 200 GPa |
🔬 Jismoniy xususiyatlar
| Mulk | Qiymat |
|---|---|
| Zichlik | 8,00 g/sm³ |
| Erish nuqtasi | 1400-1450 daraja |
| Issiqlik o'tkazuvchanligi (100 daraja) | 16.2 W/m·K |
| Issiqlik kengayish koeffitsienti (20-100 daraja) | 17.2×10-6/K |
| Maxsus issiqlik sig'imi | 500 J/kg·K |
| Elektr qarshiligi (20 daraja) | 0.72 µΩ·m |
| Magnit o'tkazuvchanlik | 1.02 (paramagnit) |
| Kyuri harorati | Magnit bo'lmagan- |