What is 1.4571 Stainless Steel?SS201 Stainless Steel Sheet304H Stainless Steel Sheet

🧪 Kimyoviy tarkibi

Element Tarkibi (%)
Uglerod (C) 0,030 dan kam yoki unga teng
Marganets (Mn) 2.00 dan kam yoki unga teng
Kremniy (Si) 0,75 dan kam yoki unga teng
Fosfor (P) 0,045 dan kam yoki unga teng
Oltingugurt (S) 0,030 dan kam yoki unga teng
Chromium (Cr) 18.00 - 20.00
Nikel (Ni) 8.00 - 12.00
Azot (N) 0,10 dan kam yoki unga teng
Temir (Fe) Balans

⚙️ Mexanik xususiyatlari

Mulk Qiymat
Mustahkamlik chegarasi 515 MPa dan katta yoki unga teng
Hosildorlik (0,2% ofset) 205 MPa dan katta yoki unga teng
50 mm gacha cho'zish 40% dan katta yoki teng
Hududning qisqarishi 50% dan katta yoki teng
Qattiqlik (Brinell) 200 HB dan kam yoki unga teng
Qattiqlik (Rockwell B) 90 HRB dan kam yoki unga teng
Ta'sir energiyasi (Charpy V-20 gradusda) 120 J dan katta yoki unga teng
Charchoq chegarasi (107tsikllar) 240 MPa
Elastiklik moduli 200 GPa

🔬 Jismoniy xususiyatlar

Mulk Qiymat
Zichlik 8,00 g/sm³
Erish nuqtasi 1400-1450 daraja
Issiqlik o'tkazuvchanligi (100 daraja) 16.2 W/m·K
Issiqlik kengayish koeffitsienti (20-100 daraja) 17.2×10-6/K
Maxsus issiqlik sig'imi 500 J/kg·K
Elektr qarshiligi (20 daraja) 0.72 µΩ·m
Magnit o'tkazuvchanlik 1.02 (paramagnit)
Kyuri harorati Magnit bo'lmagan-

📏 Mahsulot xususiyatlari

Spetsifikatsiya Mavjud variantlar
Mahsulot shakllari Choyshablar, plitalar, barlar, novdalar, quvurlar, quvurlar, rulolar, chiziqlar
Plitalar qalinligi 0,3 mm - 6.0 mm
Plitalar qalinligi 6 mm - 100 mm
Bar diametri 6 mm - 300 mm
Quvurning tashqi diametri 6 mm - 610 mm
Standartlar ASTM A240, A276, A312, EN 10088-2, JIS G4305, GB/T 3280
Yuzaki qoplamalar 2B, BA, No.4, HL (Soch chizig'i), Mirror, Tuzlangan
Tolerantlik ± 0,1 mm (qalinligi), ± 3 mm (kengligi), ± 6 mm (uzunligi)
Chet holati Tegirmon qirrasi, qirrali qirrasi, kesilgan cheti