Kimyoviy tarkibi
| 1.4006 Chelik | EN 10088-3: 2005 |
|---|---|
| Kimyoviy element | % Hozir |
| Uglerod (C) | 0.08 - 0.15 |
| Chromium (Cr) | 11.50 - 13.50 |
| Kremniy (Si) | 0.0 - 1.00 |
| Marganets (Mn) | 0.0 - 1.50 |
| Fosfor (P) | 0.0 - 0.04 |
| Oltingugurt (S) | 0.0 - 0.02 |
| Nikel (Ni) | 0.0 - 0.75 |
| Temir (Fe) | Balans |
Xususiyatlari
| Jismoniy xususiyat | Qiymat |
|---|---|
| Zichlik | 7,75 g/sm³ |
| Termal kengayish | 9.9 x 10-6/K |
| Elastiklik moduli | 300 GPa |
| Issiqlik o'tkazuvchanligi | 24.9 W/m.K |
| Elektr qarshiligi | 0.57 x 10-6Ō.m |
| Bar - Diametri 160 mm gacha yoki qalinligi | EN 10088-3: 2005 |
|---|---|
| Mexanik xususiyat | Qiymat |
| Stressni isbotlash | 450 min MPa |
| Mustahkamlik chegarasi | 650 - 850 MPa |
| Uzayish A | 15 min % |