ASTM A270 sanitariya zanglamaydigan po'latdan yasalgan naycha o'lchamlari

May 26, 2025

Xabar QOLDIRISH

NimaASTM A270 sanitariya hamkori?

ASTM A270 - bu eng yaxshi va sutli tizimlar, farmatsevtika va kosmetik qayta ishlash, ichimlik va kosmik tayyorgarlik, tez-tez mexanik polshta yoki elektropa kabi gigiena va o'lchovli aniqlik uchun standart spetsifikatsiyadir.

ASTM A270 sanitariya zanglamaydigan po'latdan yasalgan naycha o'lchami

Quyida umumiy diametr (OD) va ASTM A270 naychalari uchun umumiy diametrli (OD) mos yozuvlar jadvali. Barcha o'lchamlar bir dyuym va millimetrda.

Naycha hajmi (OD) OD (ichida) Od (mm) Devor qalinligi (ichidagi) Devor (mm) Jadval ekvivalenti
1/2" 0.500 12.70 0.065 1.65 10S \/ 16 SWG
3/4" 0.750 19.05 0.065 1.65 10S \/ 16 SWG
1" 1.000 25.40 0.065 / 0.083 1.65 / 2.11 10S \/ 14 SWG
1-1/2" 1.500 38.10 0.065 / 0.083 1.65 / 2.11 10S \/ 14 SWG
2" 2.000 50.80 0.065 / 0.109 1.65 / 2.77 10S \/ 12 SWG
2-1/2" 2.500 63.50 0.083 / 0.120 2.11 / 3.05 14 SWG \/ 11 SWG
3" 3.000 76.20 0.083 / 0.120 2.11 / 3.05 14 SWG \/ 11 SWG
4" 4.000 101.60 0.083 / 0.120 2.11 / 3.05 14 SWG \/ 11 SWG
6" 6.000 152.40 0.109 / 0.134 2.77 / 3.40 10S \/ 10 SWG

SWG=standart sim o'lchagich; 1,65 mm=~ 16 SWG; 2.11 mm=~ 14 SWG


 ASTM A270 Sanitary Tubing?

ASTM A270 sanitariya trubkasi uchun toksik

Parametr Bag'rikenglik
Tashqi diametri (OD) ± {{{0}}} 005 (± 0.13 mm)
Devor qalinligi ± 10%
Uzunlik (standart) 20 fut (6.1 m) tasodifiy yoki uzunlikka kesilgan

Sirtni tugatish variantlari (sanitariya darajasi)

Sirtni tugatish Pürüzlülülülülüraty (ra mk \/ mkm) Usul
Sf1 32 mkdan kam yoki teng (0. 8 mkm) Mexanik polyak
SF4 15 mkindan kam yoki teng (0. 4 mkm) Elektromon
SF5 \/ SF6 20 mkin yoki undan kam yoki undan kam Parlatilgan + passiverlangan \/ tozalangan

A270 naycha uchun ishlatiladigan oddiy materiallar

Moddiy baho Yo'q. Tavsif
316L S31603 Zo'r korroziya qarshiligi (afzal ko'rilgan)
304 S30400 Umumiy maqsadli zanglamaydigan
304L S30403 Yaxshiroq vindolash qobiliyati