ASTM A269 TP316L asboblar quvurlari uchun yorqin tavlangan quvurlar
May 19, 2026
Xabar QOLDIRISH
ASTM A269 TP316L zanglamaydigan po'latdan yasalgan BA trubkasi, shuningdek, toza quvur, gaz quvuri trubkasi, yuqori{2}}tozalikdagi gaz quvuri trubkasi yoki asbob trubkasi sifatida ham tanilgan, asosan, yorqin yumshatish jarayoni bilan birlashtirilgan ko'p rulonli sovuq haddeleme orqali ishlab chiqariladi. Atmosfera eritmasini nazorat ostida tozalashda{5}}trubka toza, yorqin va past-ichki va tashqi yuzalarga (Ra 0,4–0,6 mkm dan kam yoki teng) erishadi. Aniq o'lchamlari, silliq yuzalari va mukammal umumiy tozaligi bilan ichki yuza trubkalarni silliqlashdan ko'ra samaraliroq silliq silliqlash, mexanik silliqlashdan ham yaxshiroq silliqlash imkonini beradi. qoldiq va ifloslanish xavfi. Bu, ayniqsa, yuqori-tozalikdagi gaz tizimlari, analitik asboblar va o'ta yuqori tozalik standartlarini talab qiluvchi asbob quvurlari tizimlari uchun javob beradi.

Biz yetkazib beradigan ASTM A269 TP316L zanglamaydigan po'lat quvurlar sovuq-chizilgan + onlayn yorqin tavlanish jarayoni yordamida ishlab chiqariladi. Tashqi diametrli bardoshlik ± 0,05 mm ichida, bir xil devor qalinligi va mukammal partiya mustahkamligi bilan boshqarilishi mumkin. Bundan tashqari, trubka mukammal moslashuvchanlikni ta'minlaydi, bu esa kichik{7}}radiusli egilish o'rnatishni murakkab asboblar sxemalarini joylashtirish imkonini beradi. Shuningdek, u Swagelok va Norgren kabi siqish moslamalari-siz ulanishga erisha oladi, bu esa uni neft, kimyo, yarimoʻtkazgich va shunga oʻxshash sanoatlar uchun nozik asboblarni boshqarish tizimlarida keng qoʻllash imkonini beradi.
ASTM A269 TP316L yorqin tavlangan trubaning spetsifikatsiyasi
| Element | Spetsifikatsiya tafsilotlari |
|---|---|
| Mahsulot nomi | ASTM A269 TP316L Yorqin tavlangan quvur |
| Tashqi diametri (OD) | 4,76 mm - 25,4 mm (odatda 1/8 "dan 1" gacha) |
| Devor qalinligi (WT) | 0,71 mm – 2,11 mm (masalan, 16 BWG ≈ 1,65 mm) |
| Uzunlik | Mijoz talablariga muvofiq tayyorlangan; to'g'ridan-to'g'ri uzunlikdagi yoki rulon shaklida mavjud (o'ralgan quvurlar) |
| Yetkazib berish sharti | Sovuq chizilgan + yorqin tavlangan; qo'shimcha jilosiz yuqori sirt qoplamasi |
| Sinov / Tekshirish | Eddy tok sinovi (ET), gidrostatik sinov (suv bosimi sinovi) |
| Tugatish jarayoni | To'g'rilash, sobit uzunlikdagi kesish, parlatish |
| Sertifikatlar | Idoralar, ISO, MSDS; talablarga qarab ixtiyoriy PED yoki TS sertifikati |
| Qadoqlash | Belgilash/siyoh jetli bosib chiqarish, PE qoplar, so'nggi qopqoqlar, zarbadan-saqlovchi qadoqlash, changdan- himoyalangan qadoqlash |
| Ilovalar | Maxsus gaz va suyuqliklarni tashish tizimlari; EP (Elektropolished) quvurlari uchun asosiy material sifatida ham ishlatiladi |
SA269 TP316L zanglamaydigan po'lat quvurining mexanik xususiyatlari
| BAJA | CHIZILGAN Stress (MPA) MIN |
YIELD STR 0,2% ISHLAB CHIQISH (MPA) MIN |
UZOQ (% 50MM DA) MIN |
QATTIQLIK | |
|---|---|---|---|---|---|
| ROCKWELL B (HR B) MAX | BRINELL (HB) MAX | ||||
| SS 316L trubkasi | 485 | 170 | 40 | 95 | 217 |
316L zanglamas po'latdan yasalgan quvur kimyoviy tarkibi
| Material | C | MN | SI | P | S | CR | MO | NI | N | |
|---|---|---|---|---|---|---|---|---|---|---|
| SA269 TP 316L trubkasi | Min | - | - | - | - | - | 16.0 | 2.00 | 10.0 | - |
| Maks | 0.03 | 2.0 | 0.75 | 0.045 | 0.03 | 18.0 | 3.00 | 14.0 | 0.10 |
Yorqin tavlangan zanglamaydigan po'latdan choksiz quvurlarning normal o'lchami
| Oddiy o'lcham | |||||
| OD 3/16" | WT0,02" | 4,76x0,51 mm | OD3/16" | WT0,028" | 4,76x0,71 mm |
| OD3/16" | WT0,035" | 4,76x0,89 mm | OD3/16" | WT0,049" | 4,76x1,24 mm |
| OD0,24" | WT0,04" | 6x1 mm | OD0,24" | WT0,06" | 6x1,5 mm |
| OD1/4" | WT0,02" | 6,35x0,51 mm | OD1/4" | WT0,028" | 6,35x0,71 mm |
| OD1/4" | WT0,035" | 6,35x0,89 mm | OD1/4" | WT0,049" | 6,35x1,24 mm |
| OD1/4" | WT0,065" | 6,35x1,65 mm | OD5/16" | WT0,028" | 7,94x0,71 mm |
| OD5/16" | WT0,035" | 7,94x0,89 mm | OD5/16" | WT0,049" | 7,94x1,24 mm |
| OD5/16" | WT0,065" | 7,94x1,65 mm | OD3/8" | WT0,028" | 9,53x0,71 mm |
| OD3/8" | WT0,035" | 9,53x0,89 mm | OD3/8" | WT0,049" | 9,53x1,24 mm |
| OD3/8" | WT0,065" | 9,53x1,65 mm | OD0,4" | WT0,04" | 10x1 mm |
| OD0,4" | WT0,06" | 10x1,5 mm | OD0,4" | WT0,079" | 10x2 mm |
| OD0,47" | WT0,065" | 12x1 mm | OD0,47" | WT0,06" | 12x1,5 mm |
| OD1/2" | WT0,028" | 12,7x0,71 mm | OD1/2" | WT0,035" | 12,7x0,89 mm |
| OD1/2" | WT0,049" | 12,7x1,24 mm | OD1/2" | WT0,065" | 12,7x1,65 mm |
| OD0,55" | WT0,04" | 14x1 mm | OD0,55" | WT0,06" | 14x1,5 mm |
| OD5/8" | WT0,028" | 15,88x0,71 mm | OD5/8" | WT0,035" | 15,88x0,89 mm |
| OD5/8" | WT0,049" | 15,88x1,24 mm | OD5/8" | WT0,065" | 15,88x1,65 mm |
| OD5/8" | WT0,083" | 15,88x2,11 mm | OD0,63" | WT0,065" | 16x1 mm |
| OD0,63" | WT0,06" | 16x1,5 mm | OD0,63" | WT0,079" | 16x2 mm |
| OD3/4" | WT0,04" | 19,05x1 mm | OD3/4" | WT0,049" | 19,05x1,24 mm |
| OD3/4" | WT0,065" | 19,05x1,65 mm | OD3/4" | WT0,083" | 19,05x2,11 mm |
| OD1" | WT0,049" | 25,4x1,24 mm | OD1" | WT0,0665" | 25,4x1,65 mm |
| OD1" | WT0,083" | 25,4x2,11 mm | OD1" | WT0,1" | 25,4x2,54 mm |
Agar sizda aniq spetsifikatsiyalar bo'lsa, iltimos, buyurtma bering. GNEE siz tanlab olishingiz uchun-eng ko'p sotiladigan mahsulotlar inventariga ega. Iltimos, bugun fabrikamiz bilan bog'laning. Biz raqobatbardosh narxlar va mukammal xizmatni taklif qilamiz.
Bepul namuna olish uchun bosing
Bizning eksport holatimiz:
Farmatsevtika sanoati uchun tozalangan suv tizimi. GMP{1}}sertifikatlangan farmatsevtika zavodi tarqatish tizimini qurish uchun TP316L choksiz quvurlardan foydalanadi, ASTM A269 standartiga + qoʻshimcha S1 talabiga (stress bilan yumshatish), ichki yuzasi Ra 0,5 mkm dan kam yoki unga teng elektropolislangan va Practice E262 interyer sinovidan oʻtadi.
Quyida eksport mijozlarimizdan misollar keltirilgan.

GNEE zanglamaydigan po'lat mijozlar tomonidan to'g'ridan-to'g'ri tekshirishni ma'qullaydi yoki mijozlar tomonidan uchinchi tomon tekshiruv agentliklariga-tekshirish uchun topshiriladi. Biz tekshirish hujjatlarining toʻliq toʻplamini, jumladan, EN 10204 3.1 ga muvofiq ishlab chiqaruvchining sinov sertifikati (TC), xom ashyo sertifikatlari, issiqlik bilan ishlov berish/oʻlchovli buzilmaydigan sinov (HT/DNT) hisobotlari va uchinchi-shaxslarning tekshiruv hisobotlarini taqdim etamiz.
Materiallarni sinovdan o'tkazish: Barcha materiallar amaldagi standartlar va mijozlar spetsifikatsiyalariga to'liq muvofiqligini ta'minlash uchun jo'natilishdan oldin qattiq sifat nazorati sinovidan o'tadi. Sinov elementlariga quyidagilar kiradi:
1. Mexanik xususiyatni tekshirish
2. Qattiqlikni tekshirish
3. Optik emissiya spektrometriyasi (OES) kimyoviy tarkibi tahlili
4. Materiallar tarkibi tahlili (PMI)
5. Yassilash testi
6. Olovni yoqish sinovi

Bizning barcha zanglamaydigan po'latdan yasalgan choksiz quvurlarimiz har qanday shikastlanish yoki yo'qotishning oldini olish uchun xalqaro standartlarga muvofiq qadoqlangan. Odatiy bo'lib, biz qalin to'qilgan plastik qoplardan foydalangan holda tayyor quvurlarni bir-biriga bog'laymiz.
Osonlik bilan ifloslangan, tirnalgan, bosimga duchor bo'lgan yoki ishlov berish paytida oson shikastlanadigan ba'zi maxsus quvurlar uchun himoya qilish uchun yog'och qutilardan foydalanishni tavsiya etamiz. Shuni esda tutingki, yog'och quti qadoqlash qo'shimcha xarajatlarga olib keladi, jumladan, nafaqat sandiqning o'zi, balki yuk tashish xarajatlarini ham oshiradi, ayniqsa havoda yuk tashishda. Mijozlarning tajribasini yaxshilash uchun biz sizning maxsus talablaringiz bo'yicha tayyorlangan qadoqlashni ham ta'minlay olamiz.

So'rov yuborish