ASTM A269 TP316 Yorqin tavlangan zanglamaydigan po'lat quvur
May 18, 2026
Xabar QOLDIRISH
ASTM A269 TP316 yorqin tavlangan zanglamaydigan po'lat quvur TP316 (UNS S31600) materialidan tayyorlangan va Bright Annealing (BA) tomonidan qayta ishlangan ostenitik zanglamaydigan po'lat quvurdir. Odatda 16-18% xrom (Cr), 10-14% nikel (Ni) va 2-3% molibden (Mo) o'z ichiga oladi, bu mukammal korroziyaga chidamlilik, yuqori sirt qoplamasi va yaxshi mexanik xususiyatlarni ta'minlaydi.
Standart talablarga muvofiq, 316L zanglamaydigan po'lat quvurlar odatda eritma-tavlangan holda beriladi. Yuvish harorati 1040 darajadan past emas, so'ngra suvni o'chirish yoki tez sovutish bir xil mikro tuzilmani ta'minlash va granulalararo korroziyaga chidamliligini oshirish. Mahsulot choksiz va payvandlangan shakllarda mavjud bo'lib, umumiy tashqi diametrlari 6–48 mm (taxminan 1/4"–2") va devor qalinligi 0,5–3,0 mm. Standart uzunliklar 3 m, 6 m yoki moslashtirilgan o'lchamlarni o'z ichiga oladi. Sirt kumushrang oq metall yaltiroq (BA qoplamasi), tuzsiz, past pürüzlü, silliq ichki va tashqi devorlarga ega, bu tozalash va sterilizatsiya qilishni osonlashtiradi.



ASTM A269 TP316 quvurlari ichki diametri 1/4 dyuymdan katta yoki unga teng va devor qalinligi 0,020 dyuymdan katta yoki unga teng bo'lgan ilovalar uchun javob beradi. Kimyoviy, oziq-ovqat, farmatsevtika, energiya ishlab chiqarish, issiqlik almashtirgich va asbobsozlik quvurlari tizimlarida keng qo'llaniladi, bu erda yuqori tozalik va korroziyaga chidamlilik talab etiladi.
Kimyoviy tarkibi (ASTM A269 TP316)
| Element | Belgi | Tarkib (%) |
| Uglerod | C | 0,08 dan kam yoki unga teng |
| Marganets | Mn | 2.00 dan kam yoki unga teng |
| Fosfor | P | 0,045 dan kam yoki unga teng |
| Oltingugurt | S | 0,030 dan kam yoki unga teng |
| Silikon | Si | 0,75 dan kam yoki unga teng |
| Chromium | Cr | 16.0 – 18.0 |
| Nikel | Ni | 11.0 – 14.0 |
| Molibden | Mo | 2.00 – 3.00 |
sa 269 tp 316 choksiz quvur mexanik xususiyatlari
| daraja | rentabellik str (0,2% isbot) (mpa) minimal | kuchlanish str (mpa) minimal | cho'zilish (% 50 mm) minimal | qattiqlik rockwell b (soat b) maksimal | brinell (hb) maksimal |
|---|---|---|---|---|---|
| 316 | 205 | 515 | 40 | 95 | 217 |
astm a269m tp316 quvurlarining jismoniy xususiyatlari
| daraja | elastik modul (gpa) | zichlik (kg/metr3) | termal kengayishning o'rtacha ko-effisi (millimetr/m/s) 0–315 daraja c | termal kengayishning o'rtacha ko-effisi (millimetr/m/s) 0–100 daraja c | termal kengayishning o'rtacha ko-effisi (millimetr/m/s) 0–538 daraja c | solishtirma issiqlik 0-100 ° C (j/kg.k) | 100 ° C da issiqlik o'tkazuvchanligi (w/mk) | 500 ° C da issiqlik o'tkazuvchanligi (w/mk) | elektr qarshiligi (nō.m) |
|---|---|---|---|---|---|---|---|---|---|
| 316 | 193 | 8000 | 16.2 | 15.9 | 17.5 | 500 | 16.3 | 21.5 | 74 |
ASME SA 269 316 Yorqin tavlangan trubaning vazn jadvali
| Dyuymdagi tashqi diametr | 22ga .028" | 18ga .049" | 20ga ,035" | 16ga .065" | 14ga .083" | 12ga 0,109" | 25ga .020" | 28ga .010" | 13ga .095" | 11ga .120" | 9ga .148" | 10ga .134" |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 1 /2 | 8400 | 14700 | 10500 | 19500 | 24900 | 6000 | 28500 | |||||
| 0.1411 | 0.236 | 0.1738 | 0.302 | 0.3696 | 0.1025 | 0.4109 | ||||||
| 5/8 | 6725 | 11750 | 8400 | 15600 | 19925 | 4800 | 22800 | |||||
| 0.1785 | 0.3014 | 0.2205 | 0.3888 | 0.4805 | 0.1292 | 0.5377 | ||||||
| 3/4 | 5600 | 9800 | 7000 | 13000 | 16600 | 21800 | 4000 | 19000 | 24000 | |||
| 0.2159 | 0.3668 | 0.2673 | 0.4755 | 0.5913 | 0.7462 | 0.1559 | 0.6646 | 0.8074 | ||||
| 7/8 | 4800 | 8400 | 6000 | 11150 | 14250 | 18675 | 3425 | 16275 | 20570 | |||
| 0.2533 | 0.4323 | 0.314 | 0.5623 | 0.7021 | 0.8917 | 0.1826 | 0.7914 | 0.9676 | ||||
| 1 | 4200 | 7350 | 5250 | 9750 | 12450 | 16350 | 3000 | 14250 | 18000 | 22200 | 20100 | |
| 0.2907 | 0.4977 | 0.3607 | 0.6491 | 0.8129 | 1.037 | 0.2093 | 0.9182 | 1.128 | 1.347 | 1.251 | ||
| 1 -1 /4 | 3350 | 5875 | 4200 | 7800 | 9950 | 13075 | 11400 | 14400 | 17750 | 16075 | ||
| 0.3654 | 0.6285 | 0.4542 | 0.8226 | 1.034 | 1.328 | 1.172 | 1.448 | 1.742 | 1.612 | |||
| 1 -3/8 | 3050 | 5350 | 3825 | 7100 | 9050 | 11900 | 10350 | 13100 | 16150 | 14625 | ||
| 0.4028 | 0.6939 | 0.5009 | 0.9094 | 1.145 | 1.474 | 1.299 | 1.608 | 1.939 | 1.793 |
ASTM A269 standart bardoshlik
| Yo'q. | Hajmi, tashqi diametri, dyuym. | Tashqi diametrdagi ruxsat etilgan o'zgarishlar, dyuym (mm) | Devor qalinligining ruxsat etilgan o'zgarishlari,% | Kesish uzunligidagi ruxsat etilgan o'zgarishlar, dyuym (mm) | Yupqa devorli quvurlar | |
| tugadi | ostida | |||||
| 1 | ½ gacha [13] | ±0.005(0.13) | ±15 | ⅛(3.2) | 0 | ... |
| 2 | ½ dan 1½ gacha, bundan mustasno | ±0.005(0.13) | ±10 | ⅛(3.2) | 0 | nominal 0,065 dyuymdan (1,65 mm) kam |
| 3 | 1½ dan 3½ gacha, bundan mustasno | ±0.010(0.25) | ±10 | 3/16(4.8) | 0 | nominal 0,095 dyuymdan (2,41 mm) kam |
| 4 | 3½ dan 5½ gacha, bundan mustasno | ±0.015(0.38) | ±10 | 3/16(4.8) | 0 | nominal 0,150 dyuymdan (3,81 mm) kam |
| 5 | 5½ dan 8 gacha, bundan mustasno | ±0.030(0.76) | ±10 | 3/16(4.8) | 0 | nominal 0,150 dyuymdan (3,81 mm) kam |
| 6 | 8 dan 12 gacha, bundan mustasno | ±0.040(1.01) | ±10 | 3/16(4.8) | 0 | nominal 0,200 dyuymdan (5,08 mm) kam |
| 7 | 12 dan 14 gacha, bundan mustasno | ±0.050(1.26) | ±10 | 3/16(4.8) | 0 | nominal 0,220 dyuymdan (5,59 mm) kam |
ASTM A269 TP316 BA quvurlarining odatdagi sirt pürüzlülüğü (Ra) qanday?
Yorqin tavlangan (BA) quvurlarning odatdagi ichki va tashqi pürüzlülüğü, odatda, Ra<0,5 mkm (20 mikron) atrofida. Yarimo'tkazgich yoki ultra{3}}toza gaz sanoati kabi yuqori tozalikni talab qiladigan ilovalar uchun keyingi elektropolishing (EP) orqali Ra qiymatini 0,25 mkm dan pastga tushirish mumkin.
Ilovalar:
Nazorat va asboblar quvurlari.
Xromatografiya va laboratoriya jihozlari.
Farmatsevtika va biotexnologik qayta ishlash.
Yarimo'tkazgichli gaz etkazib berish tizimlari.
Dengiz va dengiz gidravlik liniyalari.
A269 darajasi TP316 sovuq chizilgan choksiz quvur HS kodi
| HS kodi | 73044100 |
|---|
Barcha mahsulotlarimiz qadoqlashdan oldin belgilangan standartlarga muvofiq individual tekshiruvdan o'tkaziladi. Faqatgina tekshiruvdan o'tganlar eksport mezonlariga muvofiq qadoqlanadi.
Yonish sinovi
Mexanik sinov
Kimyoviy sinov
Yassilash testi
PMI testi
Qattiqlik sinovi

Yetkazib berish va qadoqlash
Mahsulotlarimizning barcha mahsulotlarini turli yo'llar bilan tashish mumkin, masalan, to'liq konteyner tashish, konteyner yukidan kamroq yuk tashish, havo yuklari va boshqalar. Kompaniyamiz mijozlarning xarid xarajatlarini tejash uchun har bir buyurtma uchun optimal transport rejasini tuzadi.

So'rov yuborish