astm a249 spetsifikatsiyasi.pdf

Nov 13, 2025

Xabar QOLDIRISH

ASTM A249 standarti nima?
ASTM A249 - qozon, o'ta qizdirgich, issiqlik almashtirgich va kondensator sifatida ishlatiladigan payvandlangan ostenitik po'lat quvurlar uchun standart spetsifikatsiya. U TP304, TP304L va TP316L kabi turli navlarda mavjud bo'lgan ushbu quvurlar uchun kimyoviy va mexanik talablarni, sinovlarni va sifat nazoratini qamrab oladi. Spetsifikatsiya quvurlar uchun o'lcham oralig'ini, o'lchovli bardoshliklarni, issiqlik bilan ishlov berishni va sirtni tugatish talablarini belgilaydi.

 

ASTM A249 TP304 spetsifikatsiyasi

ASTM A249 TP304 - qozonxonalar, issiqlik almashtirgichlar va kondensatorlar kabi ilovalarda ishlatiladigan payvandlangan ostenitik zanglamaydigan po'lat quvurlar uchun spetsifikatsiya. Buning uchun 515 MPa minimal tortishish kuchi, 205 MPa minimal oqish quvvati va 50 mm gacha bo'lgan minimal cho'zilish 40% talab qilinadi. Spetsifikatsiya tekis prokat chiziqlardan ishlab chiqarilgan va toza sirt uchun tez-tez porloq tavlanadigan ushbu quvur uchun material, o'lchamlar, bardoshlik, sinov va etkazib berish shartlarini o'z ichiga oladi.

 

ASTM A249 zanglamaydigan po'latdan payvandlangan quvurlarning kimyoviy tarkibi

Baho UNS raqami. UZ No. C Cr Ni Mo Boshqalar
304 S30400 1.4301 0.08 18.00 – 20.00 8.00 – 12.00
304L S30403 1.4307 0.035 18.00 – 20.00 8.00 – 12.00
310S S31008 1.4845 0.08 24.00 – 26.00 19.00 – 22.00
316 S31620 1.4401 0.08 16.00 – 18.00 10.00 – 14.00 2.00 – 3.00
316L S31603 1.4404 0.035 16.00 – 18.00 10.00 – 14.00 2.00 – 3.00
316H S31603 0.04 – 0.10 16.00 – 18.00 10.00 – 14.00 2.00 – 3.00
316Ti S31635 1.4571 0.08 16.00 – 18.00 10.00 – 14.00 2.00 – 3.00 Ti:5X(C+N) – 0,70
317L S31703 1.4438 0.035 18.00 – 20.00 11.00 – 15.00 3.00 – 4.00
321 S32100 1.4541 0.08 17.00 – 19.00 9.00 – 12.00 Ti:5X(C+N) – 0,70
347 S34700 1.4550 0.08 16.00 – 18.00 10.00 – 14.00
347H S34709 1.4551 0.04 – 0.10 17.00 – 20.00 9.00 – 13.00

 

ASTM A249 Mexanik xususiyatlar

Material Issiqlik bilan ishlov berish Harorat F (C) Min. Qattiqlik
Brinell Rokvell
TP304 Yechim 1900 (1040) 192 HBW/200 HV 90HRB
TP304L Yechim 1900 (1040) 192 HBW/200 HV 90HRB
TP316 Yechim 1900(1040) 192 HBW/200 HV 90HRB
TP316L Yechim 1900(1040) 192 HBW/200 HV 90HRB
TP321 Yechim 1900(1040) F 192 HBW/200 HV 90HRB
TP347 Yechim 1900(1040) 192 HBW/200 HV 90HRB

 

ASTM A249 quvurlari o'lchamlari

NB O'lchami SCH 5 SCH 10 SCH 40 SCH 80 SCH 160

1/8″

available pipe tube size

available pipe tube size

available pipe tube size

available pipe tube size

 

1/4″

available pipe tube size

available pipe tube size

available pipe tube size

available pipe tube size

 

3/8″

available pipe tube size

available pipe tube size

available pipe tube size

available pipe tube size

 

1/2″

available pipe tube size

available pipe tube size

available pipe tube size

available pipe tube size

available pipe tube size

3/4″

available pipe tube size

available pipe tube size

available pipe tube size

available pipe tube size

available pipe tube size

1″

available pipe tube size

available pipe tube size

available pipe tube size

available pipe tube size

available pipe tube size

1 1/4″

available pipe tube size

available pipe tube size

available pipe tube size

available pipe tube size

available pipe tube size

1 1/2″

available pipe tube size

available pipe tube size

available pipe tube size

available pipe tube size

available pipe tube size

2″

available pipe tube size

available pipe tube size

available pipe tube size

available pipe tube size

available pipe tube size

2 1/2″

available pipe tube size

available pipe tube size

available pipe tube size

available pipe tube size

available pipe tube size

3″

available pipe tube size

available pipe tube size

available pipe tube size

available pipe tube size

available pipe tube size

4″

available pipe tube size

available pipe tube size

available pipe tube size

available pipe tube size

available pipe tube size

5″

available pipe tube size

available pipe tube size

available pipe tube size

available pipe tube size

 

6″

available pipe tube size

available pipe tube size

available pipe tube size

available pipe tube size

 

ASTM A249 issiqlik almashtirgich trubkasining tolerantliklari

Spetsifikatsiya Hajmi OD diapazoni dyuym Tolerantliklar
O.D. Devor
Bundan tashqari Minus Bundan tashqari Minus
ASTM-A-249 1000 dan past .004" .004" 10% l0%
ASME-SA-249 1000 dan 1500 gacha .006" .006" 10% 10%
Payvandlangan va sovuq ishlangan 1,501 dan 1,999 gacha .008" .008" l0% 10%
Issiqlik almashinuvi trubkasi 2000 dan 2499 gacha .010" .010" 10% 10%
O'rtacha devor 2.500 dan 2.999 gacha .012" .012" 10% 10%
(1-eslatmaga qarang) 3000 dan 4000 gacha .015" .015" 10% 10%
  4.001 dan 5.000 gacha .015" .025" 10% 10%
ASTM-A-213 1000 dan past .004" .004" 20% 0%
ASME-SA-213 1000 dan 1500 gacha .006" .005" 20% 0%
Sovuq tugallangan choksiz 1,501 dan 1,999 gacha .008" .008" 22% 0%
Issiqlik almashinuvi trubkasi 2000 dan 2499 gacha .010" .010" 22% 0%
Minimal devor 2.500 dan 2.999 gacha .012" .012" 22% 0%
(2 va 3-eslatmaga qarang) 3000 dan 4000 gacha .015" .015" 22% 0%
  4.001 dan 5.000 gacha .015" .025" 22% 0%

Eslatmalar (1) Minimal devorda ham mavjud + 18/-0%. (2) O'rtacha devorda ham mavjud ± 10% (3) Bundan tashqari, issiq ishlov berish ham mavjud, qarang

 

ASTM A249 uchun payvandlangan quvur bosimi darajasi

Welded Tube Pressure Rating For ASTM A249

ASTM A269 va A249 o'rtasidagi farq nima?
ASTM A249 payvandlashdan keyin va oxirgi issiqlik bilan ishlov berishdan oldin-payvand choki sovuq ishlov berishni talab qiladi. ASTM A269 sovuq ishlov berish yoki payvand chokini boshqarishni talab qilmaydi. ASTM A270 payvand chokini talab qilmaydi. ASTM A554 qolgan payvand choki bilan ta'minlanishi mumkin va shuning uchun u A554 ning "Boncuk olib tashlandi" opsiyasiga mos keladi.

 

ASTM A249 va A213 o'rtasidagi farq nima?
ASTM A249 - payvandlangan ostenitik po'lat qozon, o'ta qizdirgich, issiqlik almashtirgich-va kondensator quvurlari uchun standart spetsifikatsiya. ASTM A213 choksiz ferrit va ostenitik qotishma-poʻlat qozon, oʻta qizdiruvchi-almashtirgich quvurlari uchun standart xususiyatdir.

So'rov yuborish