ASTM A240 darajasi 431 DIN1.4057

Jan 14, 2026

Xabar QOLDIRISH

SUS316L Stainless Steel: Low-Carbon Corrosion Resistant GradeSUS321 Stainless Steel: Titanium-Stabilized Welding GradeSUS304 stainless steel pipe for food processing equipment

431 toifali zanglamaydigan po'latdan yasalgan kompozitsiya

Jadval 1. 431 toifali zanglamaydigan po'latlarning tarkibi diapazonlari

Baho C Mn Si P S Cr Ni
431

min.

maks.

-

0.20

-

1

-

1

-

0.04

-

0.03

15

17

1.25

2.50

 

431-sinf zanglamaydigan po'latning mexanik xususiyatlari

Jadval 2. 431-toifali zanglamaydigan po'latlarning mexanik xususiyatlari

Harorat harorati (daraja) Kuchlanish kuchi (MPa) Hosildorlik kuchi 0,2% isbot (MPa) Cho'zilish (% 50 mm) Brinell qattiqligi (HB) Impact Charpy V (J)
Tavlangan * 862 655 20 285 maksimal -
204 1345 1055 20 388 50
316 1295 1035 19 375 53
427 1350 1080 19 388 #
538 1140 965 19 321 #
593 1015 770 20 293 64

 

Sinov va hujjatlar: Zavod sinovi sertifikati, EN 10204 3.1, kimyoviy hisobot, mexanik hisobot, vayron qiluvchi sinov hisoboti,-buzuvchi sinov hisoboti, PMI sinov hisoboti, vizual tekshirish hisoboti, uchinchi-shaxs tekshiruvi hisoboti, NABL sertifikatlangan laboratoriya hisoboti.
Qadoqlash: yog'och sandiqli qadoqlash, pufakchali o'rash, po'latdan o'rash yoki mijozlar talablariga muvofiq qadoqlash.

So'rov yuborish