UNS S30908 Stainless Steel – High-Chromium Heat-Resistant Utility Alloy304L Stainless Steel Sheet for Chemical Tank Linings304L Stainless Steel Pipe for Chemical Fluid Transportation

🧪 Kimyoviy tarkibi

Element Tarkibi (%)
Uglerod (C) 0,030 dan kam yoki unga teng
Marganets (Mn) 1,20 dan kam yoki unga teng
Kremniy (Si) 0,80 dan kam yoki unga teng
Fosfor (P) 0,035 dan kam yoki unga teng
Oltingugurt (S) 0,020 dan kam yoki unga teng
Chromium (Cr) 24.0 - 26.0
Nikel (Ni) 6.0 - 8.0
Molibden (Mo) 3.0 - 5.0
Azot (N) 0.24 - 0.32
Mis (Cu) 0,50 dan kam yoki unga teng
Volfram (Vt) 0,50 dan kam yoki unga teng
Temir (Fe) Balans

⚙️ Mexanik xususiyatlari

Mulk Qiymat
Kuchlanish kuchi (Rm) 800 MPa dan katta yoki unga teng
0,2% isbot kuchi (Rp0,2) 550 MPa dan katta yoki unga teng
Uzayish (A5) 15% dan katta yoki teng
Qattiqlik (HRC) 32 dan kichik yoki teng
Ta'sir energiyasi (KV) 20 daraja 60 J dan katta yoki unga teng
Ta'sir energiyasi (KV) -40 daraja 40 J dan katta yoki unga teng
Charchoq chegarasi (10^7 tsikl) 350 MPa
Young moduli 200 GPa
Kesish moduli 80 GPa
Puasson nisbati 0.27

🔬 Jismoniy xususiyatlar

Mulk Qiymat
Zichlik 7,80 g/sm³
Erish nuqtasi 1350-1400 daraja
20 daraja issiqlik o'tkazuvchanligi 14 W/m·K
100 daraja issiqlik o'tkazuvchanligi 16 W/m·K
Termal kengayish (20-100 daraja) 13.0×10-6/K
Termal kengayish (20-300 daraja) 13.5×10-6/K
Maxsus issiqlik sig'imi 480 J/kg·K
Elektr qarshiligi 20 daraja 0.85 µΩ·m
Magnit o'tkazuvchanlik 1.02 µr
Kyuri harorati Magnit bo'lmagan-

So'rov yuborish