904L zanglamaydigan po'lat plitalarni sotib olayotganda, mavjud qalinliklar, o'lchamlar va sanoat standartlarini tushunish to'g'ri tanlov qilish uchun juda muhimdir. Bu omillar nafaqat material narxiga ta'sir qiladi, balki muayyan ilovalar, ishlab chiqarish va uzoq muddatli ishlash uchun mosligini ham belgilaydi.
904L zanglamaydigan po'lat plitalar uchun standartlar qanday?
904L zanglamaydigan po'latdan yasalgan plastinka (UNS N08904, WNR 1.4539) yuqori{3}}qotishma ostenitik zanglamaydigan po'latdir, korroziyaga mukammal qarshilikka ega bo'lib, asosan ASTM A240 va EN 10088-2 standartlariga muvofiq ishlab chiqariladi. Uning qalinligi 0,3 mm dan 100 mm gacha (sovuq haddelenmiş plitalar qalinligi 0,3-6 mm, issiq haddelenmiş plitalar qalinligi 3-100 mm va undan ko'p), standart kengligi 1000 mm, 1219 mm va 1500 mm, uzunligi 60 mm gacha.
| Standart | Spetsifikatsiya | Tavsif |
|---|---|---|
| ASTM | ASTM A240 / A240M | Issiqlikka chidamli{0}}va korroziyaga chidamli-zanglamaydigan po'lat plitalar uchun standart |
| UNS | UNS N08904 | 904L uchun yagona raqamlash tizimining belgilanishi |
| UZ | EN 1.4539 | Evropa standarti 904L ekvivalenti |
| JIS | SUS 904L | Yuqori qotishma{0}}zanglamaydigan po'lat uchun Yaponiya sanoat standarti |
| GB | GB/T 20878 | Super ostenitik zanglamaydigan po'lat plitalar uchun Xitoy standarti |
| DIN | DIN 2.4665 | Yuqori qotishma korroziyaga chidamli varaqlar uchun nemis ekvivalenti- |
904L zanglamaydigan po'lat plitalarning qalinligi
904L zanglamaydigan po'lat plitalar turli xil sanoat ehtiyojlarini qondirish uchun keng qalinlikdagi diapazonda mavjud:
904L zanglamaydigan po'latdan ultra{1}}yupqa plitalar (0,3 mm – 1 mm): nozik qismlar, dekorativ panellar va kichik-miqyosda ishlab chiqarish uchun javob beradi.
904L zanglamaydigan po'latdan yasalgan standart plitalar (1mm - 6mm): Odatda kimyoviy tanklar, quvurlar va umumiy sanoat ilovalarida qo'llaniladi.
904L zanglamaydigan po'latdan yasalgan qalin plitalar (6 mm - 20 mm): Strukturaviy qismlar, og'ir{3}}dengiz qismlari va yuqori{4}}bosimli uskunalar uchun ideal.
| Qalinligi | Hajmi diapazoni | Qalinligi | Og'irlik birligiga to'g'ri keladigan sirt maydoni | Har bir varaqning taxminan vazni | ||
|---|---|---|---|---|---|---|
| dyuym | mm | kg/m² | funt/ft² | kg | funt | |
| 0.015 | 36 x 120 | 0.381 | 3.07566 | 0.630 | 8.5617 | 18.90 |
| 0.015 | 36 x 96 | 0.381 | 3.07566 | 0.630 | 6.84936 | 15.12 |
| 0.0178 | 36 x 120 | 0.45212 | 3.690792 | 0.756 | 10.27404 | 22.68 |
| 0.0178 | 36 x 96 | 0.45212 | 3.690792 | 0.756 | 8.22195 | 18.15 |
| 0.0178 | 48 x 120 | 0.45212 | 3.690792 | 0.756 | 13.69872 | 30.24 |
| 0.0178 | 48 x 96 | 0.45212 | 3.690792 | 0.756 | 10.95807 | 24.19 |
| 0.0235 | 30 x 120 | 0.5969 | 4.921056 | 1.008 | 11.4156 | 25.20 |
| 0.0235 | 30 x 96 | 0.5969 | 4.921056 | 1.008 | 9.13248 | 20.16 |
| 0.0235 | 36 x 120 | 0.5969 | 4.921056 | 1.008 | 13.69872 | 30.24 |
SA240 904L zanglamaydigan po'latdan yasalgan plitalar
| (TAXMINCHI Dyuym) | METAL O'LCHI | NOMINAL DECIMAL (+/- Dyuym) |
| 0.1644 | 8 | 0.0080 |
| 0.1793 | 7 | 0.0080 |
| 0.1345 | 10 | 0.0070 |
| 0.1196 | 11 | 0.0050 |
| 0.1495 | 9 | 0.0080 |
| 0.1046 | 12 | 0.0050 |
| 0.0179 | 26 | 0.0015 |
| 0.0747 | 14 | 0.0040 |
| 0.0673 | 15 | 0.0040 |
| 0.0897 | 13 | 0.0050 |
| 0.0598 | 16 | 0.0030 |
| 0.0478 | 18 | 0.0030 |
SS 904L plastinka vazni jadvali
SS 904L plastinka hisoblash formulasi

| Zanglamaydigan po'latdan 904L varaqning og'irligi (kg) | Hajmi (mm) | Bir varaqning og'irligi (kg) | Hajmi (mm) |
|---|---|---|---|
| 17.9 | 2500 x1250 x 0.7 | 55.3 | 3000 x 1500 x 1.5 |
| 11.5 | 2000 x1000 x 0.7 | 38.4 | 2500 x 1250 x 1.5 |
| 14.7 | 2000 x1000 x 0.9 | 32.7 | 2000 x 1000 x 2.0 |
| 16.4 | 2000 x1000 x 1.0 | 73.7 | 3000 x 1500 x 2.0 |
| 23.0 | 2500 x1250 x 0.9 | 51.2 | 2500 x 1250 x 2.0 |
| 36.8 | 3000 x1500 x 1.0 | 63.9 | 2500 x 1250 x 2.5 |
| 25.6 | 2500 x1250 x 1.0 | 40.9 | 2000 x 1000 x 2.5 |
| 19.6 | 2000 x1000 x 1.2 | 92.1 | 3000 x 1500 x 2.5 |
| 44.2 | 3000 x1500 x 1.2 | 77.5 | 2500 x 1250 x 3.0 |
| 30.7 | 2500 x1250 x 1.2 | 49.6 | 2000 x 1000 x 3.0 |
| 24.6 | 2000 x1000 x 1.5 | 112.0 | 3000 x 1500 x 3.0 |
904L zanglamas po'latdan yasalgan plitalar ilovalari
| Sanoat | Ilova |
|---|---|
| Kimyo va neft-kimyo | Reaktorlar, tanklar, klapanlar, issiqlik almashinuvchilari |
| Dengizchi | Kema komponentlari, dengiz platformalari |
| Oziq-ovqat va ichimliklar | Yuqori darajadagi ishlov berish uskunalari- |
| Arxitektura | Yillik panellar, tutqichlar, jabhalar |
| Farmatsevtika | Saqlash idishlari, quvur tizimlari |
Yuqoridagi narsalarga talablaringiz bo'lsa, iltimos, buyurtma bering. GNEE siz tanlash uchun mashhur 904L zanglamaydigan po'lat plitalarning katta inventariga ega. Ular turli xil amaliy mahsulot shakllariga qayta ishlanishi mumkin. Batafsil kimyoviy tarkib va bepul namunalar uchun darhol fabrikamız bilan bog'laning. Biz raqobatbardosh narxlar va mukammal xizmatni taklif qilamiz.