1.4550 X6CrNiNb18-10 347 S34700 Z6CNNb18-10 347S31 2338 08KH18N12B
1.4961 X8CrNiNb16-13 347H S34709        

 

 

 

Kimyoviy xossalari:

  C Cr Mn Ni P S Si Cb/Ta
347 0,08 maksimal min: 17.0
maksimal: 20.0
2,0 maks min: 9,0
maksimal: 13.0
0,04 maksimal 0.30
maks
0.75
maks
min:10x C
maksimal: 1,0
347H min: 0,04
maksimal: 0,10
min: 17.0
maksimal: 20.0
2,0 maks min: 9,0
maksimal: 13.0
0,03 maksimal 0.30
maks
0.75
maks
min:10x C
maksimal: 1,0

 

Suface opsiyasi

1 qora yuza

2 Asoslangan: Yorqin, lekin qo'pol; Aniqlik emas

3 Plitalar uchun ishlov berish: Yorqin va aniqlik; Kichkina burilish chandig'i

4 Peeled/Torned: Yorqin va aniq; Kichkina burilish chandig'i

5 jilolangan: juda yorqin va aniq o'lcham; chandiq aylanmaydi