316L zanglamaydigan po'lat plitalar 1,0 mm sovuq haddelenmiş ASTM A240 DIN1.4404

Mar 23, 2026

Xabar QOLDIRISH

What is 1.4537 Stainless Steel?What is 1.4529 Stainless Steel?Stainless Steel - Grade 440 (UNS S44000)

Turi Zanglamaydigan po'latdan yasalgan varaq
Baho 200 seriya: 201/202
300 seriyasi: 301/302/303/304/304 L/304 N/309/309 S/310/316/316 L/321/347
400 seriyali: 403/408/409/410/416/420/430/431/440/440A/440B/440C/439/443/444
600 seriyasi: 610/620/630
900 seriyasi: 904L
Qalinligi 0,3-100 mm
Kengligi 600mm, 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm va boshqalar.
Uzunlik 2000mm, 2440mm, 3000mm, 5800mm, 6000mm va boshqalar
Yuzaki BA/2B/NO.1/NO.4/8K/HL
Sifat testi MTC, ISO, SGS, BV va boshqalarni taklif qilishimiz mumkin
To'lov shartlari L/CT/T (30% depozit)
Stok yoki yo'q Etarli zaxira
Namuna Bepul namuna
Ilova Kimyo sanoati, Tibbiyot asboblari, Qurilish materiallari, Dekorativ,
Oshxona buyumlari, oziq-ovqat va boshqalar
Yetkazib berish vaqti 7-15 kun ichida

 

 

A240 zanglamaydigan po'latdan 316L plitalar va plitalarning ekvivalent navlari

STANDART WERKSTOFF NR. UNS JIS BS GOST AFNOR UZ
SS 316L 1.4404/1.4435 S31603 SUS 316L 316S11/316S13 03Ch17N14M3 / 03Ch17N14M2 Z3CND17-11-02 / Z3CND18-14-03 X2CrNiMo17-12-2 / X2CrNiMo18-14-3

Zanglamaydigan po'latdan yasalgan 316L plitalar va plitalar kimyoviy xususiyatlari

Baho C Mn Si P S Cr Mo Ni N
SS 316L 0,035 maksimal 2,0 maks 1,00 maksimal 0,045 maks 0,030 maksimal 16 – 18 2 – 3 10 – 14 68,89 min

SS 316L Plitalar va plitalarning mexanik xususiyatlari

Zichlik Erish nuqtasi Mustahkamlik chegarasi Hosildorlik (0,2% ofset) Cho'zilish
8,0 g/sm3 1399 daraja (2550 daraja F) Psi – 75000 , MPa – 515 Psi – 30000 , MPa – 205 35 %