304L zanglamaydigan po'latdan yasalgan mahsulotlar

Mar 23, 2026

Xabar QOLDIRISH

304 Stainless Steel Pipe for Potable Water Systems304 Stainless Steel Sheet for Architectural Decoration304L Stainless Steel Coil for Marine Equipment Parts

STANDART UNS WNR. AFNOR UZ JIS BS GOST
SS 304 S30400 1.4301 Z7CN18-09 X5CrNi18-10 SUS 304 304S31 08Х18Н10
SS 304L S30403 1.4306/1.4307 Z3CN18-10 X2CrNi18-9 / X2CrNi19-11 SUS 304L 304S11 03Х18Н11
SS 304H S30409 1.4301 - - - - -

Zanglamaydigan po'latdan 304/304L/304H quvurlar va quvurlarning kimyoviy tarkibi

  C Mn Si P S Cr Ni N
304 0,07 maks 2,0 maks 0,75 maks 0,045 maks 0,03 maks min: 18,0 maksimal: 20,0 min: 8,0 maksimal: 10,5 -
304L 0,03 maks 2,0 maks 0,75 maks 0,045 maks 0,03 maks min: 18,0 maksimal: 20,0 min: 8,0 maksimal: 12,0 0,10 maks
304H min: 18.0
maksimal: 20,0
min: 8,0
maksimal: 10,5
min: 0,04
maksimal: 0,10
0.75
maks
2.0
maks
0.045
maks
0.03
maks
0.10
maks

Zanglamaydigan po'latdan yasalgan 304/304L/304H quvurlar va quvurlarning mexanik xususiyatlari

Baho Kuchlanish kuchi ksi (min) Hosildorlik kuchi 0,2% ksi (min) Uzayish % Qattiqlik (Brinell) MAX Qattiqlik (Rokvell B) MAX
304 75 30 40 201 92
304L 70 25 40 201 92
304H 75 30 40 201 92