Mijoz uchun 15-5PH zanglamaydigan po'latdan yasalgan bar, plastinka va choyshab

Mar 16, 2026

Xabar QOLDIRISH

What is 1.4028 Stainless Steel?410 Stainless Steel Plate | Sheet304H Stainless Steel Sheet

Standart

AMS 5659, AMS 5823, AMS 5862, ASTM A564 / A564M, ASTM A693

Baho

0Cr15Ni5Cu4Nb, 1.4545, S15500

Uzunlik

1000 mm-6000 mm (39,37-236,22 dyuym), moslashtirilgan

Diametri

Bar: 6 mm-300 mm (0,24-12 dyuym), moslashtirilgan

Qalinlik

Moslashtirilgan, Plitalar: 6 mm-100 mm (0,24-3,94 dyuym), varaq: 0,5 mm-6 mm (0,02-0,24 dyuym)

To'liq kenglik

Moslashtirilgan, varaq va plastinka: 1000 mm-2000 mm (39,37-78,74 dyuym)

Yuzaki tugatish

2B, 2D, BA, Qoplangan va h.k., Maydalangan, Tegirmon, №1, №4, Tozalangan, Sayqallangan, Tornalangan

Shakl

15-5PH soxta bar, 15-5PH plastinka, 15-5PH sayqallangan plastinka, 15-5PH varaq, 15-5PH temperli varaq, lasan, sovuq chizilgan bar, sovuq haddelenmiş plastinka va boshqalar, tekis bar, issiq haddelenmiş varaq, to'rtburchak novda, novda, dumaloq

 

Kimyoviy birikmalar

Chromium (Cr)Nikel (Ni)Mis (Cu)Marganets (Mn)Kremniy (Si)Uglerod (C)Fosfor (P)Oltingugurt (S)Azot (N)
         
14,0 - 15,53,5 – 5,52,5 – 4,51,0 maks1,0 maks0,07 maksimal0,04 maksimal0,03 maksimal0,10 maks

Mexanik xususiyatlar

XususiyatlariMetrik birlikImperator birligi
   
Mustahkamlik chegarasi1000-1170 MPa145-170 ksi
Hosildorlik kuchi≥ 1000 MPa≥ 145 ksi
Vickers qattiqligi360 HV (odatiy)360 HV (odatiy)
Brinell qattiqligi350 HB (odatiy)350 HB (odatiy)
Rokvellning qattiqligi35 HRC (odatiy)35 HRC (odatiy)
Cho'zilish≥ 10%≥ 10%
Elastik modul200 GPa29,0 x 10³ ksi

So'rov yuborish