| Standart |
AMS 5659, AMS 5823, AMS 5862, ASTM A564 / A564M, ASTM A693 |
|---|---|
| Baho |
0Cr15Ni5Cu4Nb, 1.4545, S15500 |
| Uzunlik |
1000 mm-6000 mm (39,37-236,22 dyuym), moslashtirilgan |
| Diametri |
Bar: 6 mm-300 mm (0,24-12 dyuym), moslashtirilgan |
| Qalinlik |
Moslashtirilgan, Plitalar: 6 mm-100 mm (0,24-3,94 dyuym), varaq: 0,5 mm-6 mm (0,02-0,24 dyuym) |
| To'liq kenglik |
Moslashtirilgan, varaq va plastinka: 1000 mm-2000 mm (39,37-78,74 dyuym) |
| Yuzaki tugatish |
2B, 2D, BA, Qoplangan va h.k., Maydalangan, Tegirmon, №1, №4, Tozalangan, Sayqallangan, Tornalangan |
| Shakl |
15-5PH soxta bar, 15-5PH plastinka, 15-5PH sayqallangan plastinka, 15-5PH varaq, 15-5PH temperli varaq, lasan, sovuq chizilgan bar, sovuq haddelenmiş plastinka va boshqalar, tekis bar, issiq haddelenmiş varaq, to'rtburchak novda, novda, dumaloq |
Biznes shartlari
| Shartlar | Spetsifikatsiya |
|---|---|
| Minimal buyurtma miqdori: | 5 tonna |
| Narxi: | Muzokaralar olib borish uchun |
| Qadoqlash tafsilotlari: |
Talab qilinganidek |
| Yetkazib berish vaqti: | 7-10 ish kuni ichida |
| To'lov shartlari: | T/T, L/C, kredit karta |
| Ta'minot qobiliyati: | Oyiga 100 000 tonna |
| Sertifikatlash: | RoHS, BIS, SABS, tisi, KS, JIS, ISO9001 |
| Eksport qilish: |
Qo'shma Shtatlar, Frantsiya, Yaponiya, Germaniya, Italiya, Ispaniya, Buyuk Britaniya, Tayvan, Turkiya, Koreya, Braziliya, Avstriya, Niderlandiya, Meksika, Hindiston, Polsha, Vetnam, Rossiya Federatsiyasi va boshqalar. |
So'rov yuborish